Mathias
Mathias
01:32 Nov-09-2005
EN Standard for wire IQI

Hi
Does anyone know which EN Standard covers/describes the wire iqi´s?


 
 Reply 
 
Uli Mletzko
R & D, Retired
Germany, Joined Nov 1998, 89

Uli Mletzko

R & D, Retired
Germany,
Joined Nov 1998
89
09:32 Nov-11-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: Hi
: Does anyone know which EN Standard covers/describes the wire iqi´s?
------------ End Original Message ------------

Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.

Regards
Uli Mletzko
MPA, University of Stuttgart
(Germany)




 
 Reply 
 
Kaveh
Kaveh
07:26 Nov-14-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: : Hi
: : Does anyone know which EN Standard covers/describes the wire iqi?s?
: Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.
: Regards
: Uli Mletzko
: MPA, University of Stuttgart
: (Germany)
------------ End Original Message ------------

Dear Uli
Detail of IQI construction in EN-462-5-1996.
EN 462-1-1994 shows typical construction details of one design.
Tables of acceptable wire diameters for different specimen thickness are given in EN 462-3, EN 462-4 and EN 1435-1997.
This type of IQI is shown in detail in EN 462-2-1994
Tables of IQI sensitivities for the IQI on the film side are included in EN 1453-1997 and EN 462-3-1997.

Regards
Kaveh Edalati


 
 Reply 
 

Product Spotlight

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window