Technical Discussions
Mathias
Mathias
01:32 Nov-09-2005
EN Standard for wire IQI

Hi
Does anyone know which EN Standard covers/describes the wire iqi´s?


 
 Reply 
 
Uli Mletzko
R & D, Retired
Germany, Joined Nov 1998, 89

Uli Mletzko

R & D, Retired
Germany,
Joined Nov 1998
89
09:32 Nov-11-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: Hi
: Does anyone know which EN Standard covers/describes the wire iqi´s?
------------ End Original Message ------------

Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.

Regards
Uli Mletzko
MPA, University of Stuttgart
(Germany)




 
 Reply 
 
Kaveh
Kaveh
07:26 Nov-14-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: : Hi
: : Does anyone know which EN Standard covers/describes the wire iqi?s?
: Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.
: Regards
: Uli Mletzko
: MPA, University of Stuttgart
: (Germany)
------------ End Original Message ------------

Dear Uli
Detail of IQI construction in EN-462-5-1996.
EN 462-1-1994 shows typical construction details of one design.
Tables of acceptable wire diameters for different specimen thickness are given in EN 462-3, EN 462-4 and EN 1435-1997.
This type of IQI is shown in detail in EN 462-2-1994
Tables of IQI sensitivities for the IQI on the film side are included in EN 1453-1997 and EN 462-3-1997.

Regards
Kaveh Edalati


 
 Reply 
 

Product Spotlight

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window