Mathias
Mathias
01:32 Nov-09-2005
EN Standard for wire IQI

Hi
Does anyone know which EN Standard covers/describes the wire iqi´s?


 
 Reply 
 
Uli Mletzko
R & D, Retired
Germany, Joined Nov 1998, 89

Uli Mletzko

R & D, Retired
Germany,
Joined Nov 1998
89
09:32 Nov-11-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: Hi
: Does anyone know which EN Standard covers/describes the wire iqi´s?
------------ End Original Message ------------

Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.

Regards
Uli Mletzko
MPA, University of Stuttgart
(Germany)




 
 Reply 
 
Kaveh
Kaveh
07:26 Nov-14-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: : Hi
: : Does anyone know which EN Standard covers/describes the wire iqi?s?
: Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.
: Regards
: Uli Mletzko
: MPA, University of Stuttgart
: (Germany)
------------ End Original Message ------------

Dear Uli
Detail of IQI construction in EN-462-5-1996.
EN 462-1-1994 shows typical construction details of one design.
Tables of acceptable wire diameters for different specimen thickness are given in EN 462-3, EN 462-4 and EN 1435-1997.
This type of IQI is shown in detail in EN 462-2-1994
Tables of IQI sensitivities for the IQI on the film side are included in EN 1453-1997 and EN 462-3-1997.

Regards
Kaveh Edalati


 
 Reply 
 

Product Spotlight

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>