Hi everybody,

I just got my new search unit of one inch large but now I need to know if i can check my sound entry point with the IIW block "type one" and if not what should i do?

Thanks


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
01:10 Nov-11-2005
Re: Search unit
Its been a week since you posted, so I hope you managed to check the probe's emission index, Louis.

You do not specify exactly which type of probe you have, but lets say its a 2MHz 1" diameter, 60 deg shearwave. The IIW block (V1) is 25mm thick with a radius of 100mm. This should be ideal for checking the beam emission (index) point. If you are concerned about the probe housing being larger than the block thickness, put two blocks together, they make a 50 mm thcickness..

Best regards

Nigel

----------- Start Original Message -----------
: Hi everybody,
: I just got my new search unit of one inch large but now I need to know if i can check my sound entry point with the IIW block "type one" and if not what should i do?
: Thanks
------------ End Original Message ------------




 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 182

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
182
01:27 Nov-14-2005
Re: Search unit
reply by Udo Schlengermann:

Two effects cause unacceptable inaccuracies when checking large sized angle-beam-probes on the IIW calibration block (25 mm thick, 100 mm quadrant):

1. side-wall reflections have influence on the pulse shape, i.e. on the maximum echo. So the position of maximum echo amplitude will not necessarily be the one where the beam hits the quadrant surface radially.

2. depending on the frequency the near-field length of a large probe may be larger than the radius of the quadrant (100 mm). Then the maxium echo is disturbed by near-field interferences. So determination of the index point (and beam angle) may be not correct.

Contrary to the reply by Nigel Armstrong, I cannot recommend the use of two parallel 25-mm-blocks, because the interface between the blocks will still cause side wall reflections.

Because of these reasons European Standard EN 12223 on block no 1 allows for modifications (thicker blocks).
European Standard 12668-2 for verfication of probes in annex B for example shows a modification with a thickness of 100 mm.

If your probe has a nearfield in steel larger than 100 mm, you have to use special blocks with a radius larger than that nearfield. Only then the axis of the beam hits the quadrant suface radially at the point of maximum echo amplitude.
Manufacturer's verification has to use blocks with radius up to 200 mm , as required by EN 12668-2.

Kind regards
Udo Schlengermann
Applications Laboratory
GE Inspection Technologies GmbH
Huerth, Germany


----------- Start Original Message -----------
: Hi everybody,
: I just got my new search unit of one inch large but now I need to know if i can check my sound entry point with the IIW block "type one" and if not what should i do?
: Thanks
------------ End Original Message ------------




 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
04:12 Nov-15-2005
Re: Search unit
I stand corrected. A practice derived from that usual problem out in the field - lack of resources. Thank you, Udo, for your clear explanation. I shall tell my employers: "Give me the right tools and I shall do my best to give give you a quality result."


 
 Reply 
 

Product Spotlight

Content on Demand by Eddyfi Technologies

Finding yourself in front of a screen practicing safe social distancing instead of out in the fiel
...
d? At Eddyfi Technologies, we are doing our part in helping you be better prepared for what comes next. We introduce to you Eddyfi on Demand. Fill your schedule with webinars, how-to videos, informative technical papers and our NEW addition: Eddyfi Academy. There, you will have access to FREE online courses and obtain certificates of attendance once completed in order for you to include these e-learning sessions in your log of required training hours. Join us today. Stay safe, stay Beyond Current.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window