where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

1267 views
Technical Discussions
RT. JEYAKUMAR
NDT Inspector
Singapore, Joined Aug 2002, 10

RT. JEYAKUMAR

NDT Inspector
Singapore,
Joined Aug 2002
10
09:50 Nov-29-2005
CHIME TECHNIQUE

Dear Sir,

Is that chime technique use of both shear wave angle along with surface wave. If so, there is chance missing flaws on the back surface, since surface wave could not travel through.

Can anyone please kindly explain about it?

Thank you very much

With regards,

RT. Jeyakumar


 
 Reply 
 
Alan Maclean
Alan Maclean
05:00 Dec-06-2005
Re: CHIME TECHNIQUE
----------- Start Original Message -----------
: Dear Sir,
: Is that chime technique use of both shear wave angle along with surface wave. If so, there is chance missing flaws on the back surface, since surface wave could not travel through.
: Can anyone please kindly explain about it?
: Thank you very much
: With regards,
: RT. Jeyakumar

The CHIME technique as it names suggests has creeping waves propagating along the top and inner surfaces which in turn generate headwaves between the inner and outer surfaces.

Regards

Alan Maclean


------------ End Original Message ------------




 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
03:58 Dec-06-2005
Re: CHIME TECHNIQUE
I have not heard of the CHIME Technique? Then I see the mention to what looks like ID and OD Creeping Waves. Then I see a reference to Shear Waves with Surface Waves.

Is the CHIME Technique another name for the Creeping Technique that we usually reference as ID Creeping Waves. These are the result of Mode Conversions that take palce at the ID or Opposite Surface which is the scanning surface.

Is the CHIME an acronym? Is so, what does it mean?

Sincerely,

J. Mark Davis
----------- Start Original Message -----------
: : Dear Sir,
: : Is that chime technique use of both shear wave angle along with surface wave. If so, there is chance missing flaws on the back surface, since surface wave could not travel through.
: : Can anyone please kindly explain about it?
: : Thank you very much
: : With regards,
: : RT. Jeyakumar
: The CHIME technique as it names suggests has creeping waves propagating along the top and inner surfaces which in turn generate headwaves between the inner and outer surfaces.
: Regards
: Alan Maclean
:
------------ End Original Message ------------




 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
09:31 Dec-07-2005
Re: CHIME TECHNIQUE
Hello Mark

A blurb appears in December's Insight - "A new approach to pipe and vessel inspection for corrosion and cracking" for Veritec Sonomatic's CHIME service. It says CHIME is Creeping Headwave Inspection MEthodology. and uses a combination of ultrasonic headwaves and creeping waves, plus pulse-echo backscatter reflective techniques. It appears to be qualitative rather than quantitaive as it is claimed the system can differentiate material thinning into three categories, <10%t, 10-40%t and >40%t.

Hope this helps

regards

Nigel


----------- Start Original Message -----------
: I have not heard of the CHIME Technique? Then I see the mention to what looks like ID and OD Creeping Waves. Then I see a reference to Shear Waves with Surface Waves.
: Is the CHIME Technique another name for the Creeping Technique that we usually reference as ID Creeping Waves. These are the result of Mode Conversions that take palce at the ID or Opposite Surface which is the scanning surface.
: Is the CHIME an acronym? Is so, what does it mean?
: Sincerely,
: J. Mark Davis
: : : Dear Sir,
: : : Is that chime technique use of both shear wave angle along with surface wave. If so, there is chance missing flaws on the back surface, since surface wave could not travel through.
: : : Can anyone please kindly explain about it?
: : : Thank you very much
: : : With regards,
: : : RT. Jeyakumar
: : The CHIME technique as it names suggests has creeping waves propagating along the top and inner surfaces which in turn generate headwaves between the inner and outer surfaces.
: : Regards
: : Alan Maclean
: :
------------ End Original Message ------------




 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
03:53 Dec-08-2005
Re: CHIME TECHNIQUE
To All,

To add to Paul's comments:

The High Angle L-Wave with the Creeping Wave Technique can be calibrated for a Time of FLight (TOF)measurement which can provide a quantative depth or crack height measurement.

(Note: I have used only the Creeping Wave Method three (3) times to pass the EPRI NDE Center Crack Sizing Exam to show it can be a quantative method. I will add that it is "normally" a qualitative method for crack sizing as Paul mentioned. All this is really based upon the critical flaw depth)

In addition to the TOF L-wave, the echo dynamnics of the mode converted signal (Shear wave mode converted to an L Wave, and reflected as an L Wave, called CE-1) is a very useful piece of data for crack depth measurments. This is qualitattvie

To conlcude, it is the combination of absence or presence of the 3 signals (L-wave, CE-1 and CE-2) as well as echo dynamics and the TOF of the High Angle L-wave that provide qualitative or quantative crack height information.

Calibration is conducted on a block of similar material type as the component as to be examined, with notches of varying depth, i.e., 20 %, 40 %, 60 %, and 80 %. A signal pattern is observed from each notch and a comparison is made from the notches to the crack. This can be a subjective or objective analysis.

Please go to the ndt.net publications section to view the intorductory chapter from the Handbook on Advanced UT Flaw Sizing. This will expalin the wave physics assoiated with using Creeping waves.

I myself will be speaking with Paul about his probe designs using creeping waves for a CHIME Technique.

Sincerely,

J. Mark Davis

----------- Start Original Message -----------
: Hello Mark
: A blurb appears in December's Insight - "A new approach to pipe and vessel inspection for corrosion and cracking" for Veritec Sonomatic's CHIME service. It says CHIME is Creeping Headwave Inspection MEthodology. and uses a combination of ultrasonic headwaves and creeping waves, plus pulse-echo backscatter reflective techniques. It appears to be qualitative rather than quantitaive as it is claimed the system can differentiate material thinning into three categories, <10%t, 10-40%t and >40%t.
: Hope this helps
: regards
: Nigel
:
: : I have not heard of the CHIME Technique? Then I see the mention to what looks like ID and OD Creeping Waves. Then I see a reference to Shear Waves with Surface Waves.
: : Is the CHIME Technique another name for the Creeping Technique that we usually reference as ID Creeping Waves. These are the result of Mode Conversions that take palce at the ID or Opposite Surface which is the scanning surface.
: : Is the CHIME an acronym? Is so, what does it mean?
: : Sincerely,
: : J. Mark Davis
: : : : Dear Sir,
: : : : Is that chime technique use of both shear wave angle along with surface wave. If so, there is chance missing flaws on the back surface, since surface wave could not travel through.
: : : : Can anyone please kindly explain about it?
: : : : Thank you very much
: : : : With regards,
: : : : RT. Jeyakumar
: : : The CHIME technique as it names suggests has creeping waves propagating along the top and inner surfaces which in turn generate headwaves between the inner and outer surfaces.
: : : Regards
: : : Alan Maclean
: : :
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window