prakash
prakash
04:59 Jan-21-2006
NDT of fastner head

can the head of a fastner be tested for crack after forging using some NDT method? If so how?


 
 Reply 
 
P V SASTRY
P V SASTRY
00:15 Jan-22-2006
Re: NDT of fastner head
----------- Start Original Message -----------
: can the head of a fastner be tested for crack after forging using some NDT method? If so how?
------------ End Original Message ------------
They can be very easily tested for the presence of cracks/bursts using wet fluorescent magnetic particle testing(WFMPT),assuming that the fasteners are of ferromagnetic material. This is a fast and reliable method that will detect cracks of even a few microns width when properly applied. Alternately Dye Penetrant testing(PT) also can be used as a stop gap arrangement before you can procure the preffered WFMPT set up.In case the fastners are of non ferromagnetic materials like SS, PT (colour/fluorescent)can only be aplied.



 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
06:05 Jan-23-2006
Re: NDT of fastner head
----------- Start Original Message -----------
: can the head of a fastner be tested for crack after forging using some NDT method? If so how?
------------ End Original Message ------------

Dear Prakash,

Yes, there are several options. Magnetic Particle Testing is one (I am assuming that the fastener is magnetic). If you need real time high speed testing, you should think of automated UT and or RT. If you can accept batch testing mode, MT and PT (if non-magnetic material is invoved) may be good enough.

Swamy

Swamy



 
 Reply 
 

Product Spotlight

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window