RT of thin sheet welds

Hello,

I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?

Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?

S S Ananthan


 
 Reply 
 
Fred
Fred
02:47 Mar-06-2006
Re: RT of thin sheet welds
----------- Start Original Message -----------
: Hello,
: I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?
: Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?
: S S Ananthan
------------ End Original Message ------------

What would you use for penetrameters?



 
 Reply 
 
S S Ananthan
Consultant,
RAA Tech Solutions, India, Joined Jun 2000, 36

S S Ananthan

Consultant,
RAA Tech Solutions,
India,
Joined Jun 2000
36
00:08 Mar-16-2006
Re: RT of thin sheet welds
----------- Start Original Message -----------
: : Hello,
: : I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?
: : Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?
: : S S Ananthan
: What would you use for penetrameters?
------------ End Original Message ------------

We can use wire penetrameters - whatever is the minimum diameter available. The sensitiuvity will not be definitely 2% but at least some testing is possible .
My question : 1) Is RT required ? 2) Is any standard available for such requirements?


S S Ananthan





 
 Reply 
 
Jaromir A. Masa, PhD
Jaromir A. Masa, PhD
00:05 Mar-17-2006
Re: RT of thin sheet welds

The main question is, why they require x-ray testing. What will flow inside? And how the tin sheet weld seam will be stressed. I remember, in chemical industry, the tubes with liquid ethylene were 100% x-rayed. Stress was in cryogenic temperatures. When you speak about hydro a pressure testing, it is clear, it concerns low-dia tubes. Another question are the dimensions of allowable flaws.

Jaromir Amadeus Masa
Starmans Electronics Ltd
Prague



 
 Reply 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window