RT of thin sheet welds

Hello,

I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?

Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?

S S Ananthan


 
 Reply 
 
Fred
Fred
02:47 Mar-06-2006
Re: RT of thin sheet welds
----------- Start Original Message -----------
: Hello,
: I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?
: Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?
: S S Ananthan
------------ End Original Message ------------

What would you use for penetrameters?



 
 Reply 
 
S S Ananthan
Consultant,
RAA Tech Solutions, India, Joined Jun 2000, 36

S S Ananthan

Consultant,
RAA Tech Solutions,
India,
Joined Jun 2000
36
00:08 Mar-16-2006
Re: RT of thin sheet welds
----------- Start Original Message -----------
: : Hello,
: : I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?
: : Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?
: : S S Ananthan
: What would you use for penetrameters?
------------ End Original Message ------------

We can use wire penetrameters - whatever is the minimum diameter available. The sensitiuvity will not be definitely 2% but at least some testing is possible .
My question : 1) Is RT required ? 2) Is any standard available for such requirements?


S S Ananthan





 
 Reply 
 
Jaromir A. Masa, PhD
Jaromir A. Masa, PhD
00:05 Mar-17-2006
Re: RT of thin sheet welds

The main question is, why they require x-ray testing. What will flow inside? And how the tin sheet weld seam will be stressed. I remember, in chemical industry, the tubes with liquid ethylene were 100% x-rayed. Stress was in cryogenic temperatures. When you speak about hydro a pressure testing, it is clear, it concerns low-dia tubes. Another question are the dimensions of allowable flaws.

Jaromir Amadeus Masa
Starmans Electronics Ltd
Prague



 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>