01:19 Mar-06-2006
RT of thin sheet welds

Hello,

I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?

Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?

S S Ananthan


 
 Reply 
 
Fred
Fred
02:47 Mar-06-2006
Re: RT of thin sheet welds
----------- Start Original Message -----------
: Hello,
: I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?
: Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?
: S S Ananthan
------------ End Original Message ------------

What would you use for penetrameters?



 
 Reply 
 
S S Ananthan
Consultant,
RAA Tech Solutions, India, Joined Jun 2000, 36

S S Ananthan

Consultant,
RAA Tech Solutions,
India,
Joined Jun 2000
36
00:08 Mar-16-2006
Re: RT of thin sheet welds
----------- Start Original Message -----------
: : Hello,
: : I have been asked to take radiographs of thin sheet SS welds - 0.5 mm and above. Is there any requirement for RT of such a low thickness ? Will not a hydrotest adn PT be sufficiient for this purpose ?
: : Is there any standard for RT of such thin sheets ? What would be the possible sensitivity acheivable in X rays ?
: : S S Ananthan
: What would you use for penetrameters?
------------ End Original Message ------------

We can use wire penetrameters - whatever is the minimum diameter available. The sensitiuvity will not be definitely 2% but at least some testing is possible .
My question : 1) Is RT required ? 2) Is any standard available for such requirements?


S S Ananthan





 
 Reply 
 
Jaromir A. Masa, PhD
Jaromir A. Masa, PhD
00:05 Mar-17-2006
Re: RT of thin sheet welds

The main question is, why they require x-ray testing. What will flow inside? And how the tin sheet weld seam will be stressed. I remember, in chemical industry, the tubes with liquid ethylene were 100% x-rayed. Stress was in cryogenic temperatures. When you speak about hydro a pressure testing, it is clear, it concerns low-dia tubes. Another question are the dimensions of allowable flaws.

Jaromir Amadeus Masa
Starmans Electronics Ltd
Prague



 
 Reply 
 

Product Spotlight

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window