02:09 Mar-20-2006
UT Flaw detection in Monel and Hastelloy weldments

Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.

Kind Regards Charlie


 
 Reply 
 
Frank
Frank
05:35 Mar-25-2006
Re: UT Flaw detection in Monel and Hastelloy weldments
----------- Start Original Message -----------
: Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.
: Kind Regards Charlie
------------ End Original Message ------------

Try using Refracted Longitudinal search units.


 
 Reply 
 
Jim Knowles
Jim Knowles
00:12 Mar-28-2006
Re: UT Flaw detection in Monel and Hastelloy weldments
----------- Start Original Message -----------
: : Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.
: : Kind Regards Charlie
: Try using Refracted Longitudinal search units.
------------ End Original Message ------------


The corrosion of this type can be put into three categories,notch, U type or escarpment, two can be detected relatively easily by a 45 degree shear either 0.5 skip or multiple skip paying attention to the particular area of impingement or beam path length. The escarpment type of geometry is more difficult as it is shallow from the pipe side gradually getting deeper nearer the weld or HAZ. Try using 4.0 MHz shear or if the material is partcularly noisy angled compression as Charlie recommends.



 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
04:21 Mar-28-2006
Re: UT Flaw detection in Monel and Hastelloy weldments
IS this just corrosion or is ID cracking a concern.

Refracted Longitudinal Waves may work and even ID Creeping Waves.

Phased Array UT is another consideration. Either a E Scan or a S-Scan could image the sorroded area.

Is there any weld crown restriction?

How thick is the Hastelloy and Monel material?

J. Mark Davis

----------- Start Original Message -----------
: : Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.
: : Kind Regards Charlie
: Try using Refracted Longitudinal search units.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>