UT Flaw detection in Monel and Hastelloy weldments

Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.

Kind Regards Charlie


 
 Reply 
 
Frank
Frank
05:35 Mar-25-2006
Re: UT Flaw detection in Monel and Hastelloy weldments
----------- Start Original Message -----------
: Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.
: Kind Regards Charlie
------------ End Original Message ------------

Try using Refracted Longitudinal search units.


 
 Reply 
 
Jim Knowles
Jim Knowles
00:12 Mar-28-2006
Re: UT Flaw detection in Monel and Hastelloy weldments
----------- Start Original Message -----------
: : Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.
: : Kind Regards Charlie
: Try using Refracted Longitudinal search units.
------------ End Original Message ------------


The corrosion of this type can be put into three categories,notch, U type or escarpment, two can be detected relatively easily by a 45 degree shear either 0.5 skip or multiple skip paying attention to the particular area of impingement or beam path length. The escarpment type of geometry is more difficult as it is shallow from the pipe side gradually getting deeper nearer the weld or HAZ. Try using 4.0 MHz shear or if the material is partcularly noisy angled compression as Charlie recommends.



 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
04:21 Mar-28-2006
Re: UT Flaw detection in Monel and Hastelloy weldments
IS this just corrosion or is ID cracking a concern.

Refracted Longitudinal Waves may work and even ID Creeping Waves.

Phased Array UT is another consideration. Either a E Scan or a S-Scan could image the sorroded area.

Is there any weld crown restriction?

How thick is the Hastelloy and Monel material?

J. Mark Davis

----------- Start Original Message -----------
: : Interested to know of any UT Techniques for Monel or Hastelloy weldments which would give a reasonable POD for preferential ID corrosion loss to Weld or HAZ in piping.
: : Kind Regards Charlie
: Try using Refracted Longitudinal search units.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window