01:06 Apr-11-2006
measuring conductivity and permeability

Dear all,

We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples. The samples typically have a flat site a few cm across. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?

Best regards


 
 Reply 
 
Linas Svilainis
R & D,
Kaunas University of Technology, Lithuania, Joined Nov 1998, 68

Linas Svilainis

R & D,
Kaunas University of Technology,
Lithuania,
Joined Nov 1998
68
02:25 Apr-11-2006
Re: measuring conductivity and permeability
Dear Elmar,

you wrote
----------- Start Original Message -----------
: ..We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples...

Maybe it's a complex permeability you want to measure?
If yes:

.. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?...

Then RLC meter with some mathematics on geometry will do. We have prepared the paper on toroidal samples complex permeability measurement in low frequency range (0.1-10MHz). If interested, I can send you some excerpts.

People do complex permeability measurement at GHz. For instance, refer to:
Jacquart. Influence of the electrical resistivity of a ferromagnetic thin film on its permeability measurement performed with a permeameter. Elsevier Journal of Magnetism and Magnetic Materials 281 (2004) 82–91

Best regards

Linas


 
 Reply 
 
Changqing Lee
Changqing Lee
03:37 Apr-11-2006
Re: measuring conductivity and permeability
I have seen people use alternative current potential drop (ACPD) method for measuring the electrical conductivity and the effective magnetic permeability of ferromagnatic samples at the frequency range of several hundred Hz to 10KHz. Please google it yourself.

Eddy current testing is another option. But to determine conductivity and permeability at the same time is always hard.

----------- Start Original Message -----------
: Dear Elmar,
: you wrote
: : ..We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples...
: Maybe it's a complex permeability you want to measure?
: If yes:
: .. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?...
: Then RLC meter with some mathematics on geometry will do. We have prepared the paper on toroidal samples complex permeability measurement in low frequency range (0.1-10MHz). If interested, I can send you some excerpts.
: People do complex permeability measurement at GHz. For instance, refer to:
: Jacquart. Influence of the electrical resistivity of a ferromagnetic thin film on its permeability measurement performed with a permeameter. Elsevier Journal of Magnetism and Magnetic Materials 281 (2004) 82–91
: Best regards
: Linas
------------ End Original Message ------------




 
 Reply 
 
Jim Yukes
Consultant
Canada, Joined Aug 2005, 11

Jim Yukes

Consultant
Canada,
Joined Aug 2005
11
08:15 Apr-13-2006
Re: measuring conductivity and permeability
I checked with a Queens U Magnetics Department Grad & he suggested: There are many different ways to measure permeability depending on the material and application. For some standard methods visit www.astm.org and search for standards with key words "magnetic permeability".

For the conductivity measurement, Google search phrase "contact resistance tester".

----------- Start Original Message -----------
: Dear all,
: We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples. The samples typically have a flat site a few cm across. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?
: Best regards
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window