where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

WesDyne International (AMDATA Products)
WesDyne is an engineering and technical services firm dedicated to providing standard and custom nondestructive examinations (NDE) products and systems
1720 views
Technical Discussions
Elmar van den Elzen
Engineering,
Lismar Engineering B.V., Netherlands, Joined Aug 2000, 15

Elmar van den Elzen

Engineering,
Lismar Engineering B.V.,
Netherlands,
Joined Aug 2000
15
01:06 Apr-11-2006
measuring conductivity and permeability

Dear all,

We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples. The samples typically have a flat site a few cm across. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?

Best regards


 
 Reply 
 
Linas Svilainis
R & D,
Kaunas University of Technology, Lithuania, Joined Nov 1998, 67

Linas Svilainis

R & D,
Kaunas University of Technology,
Lithuania,
Joined Nov 1998
67
02:25 Apr-11-2006
Re: measuring conductivity and permeability
Dear Elmar,

you wrote
----------- Start Original Message -----------
: ..We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples...

Maybe it's a complex permeability you want to measure?
If yes:

.. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?...

Then RLC meter with some mathematics on geometry will do. We have prepared the paper on toroidal samples complex permeability measurement in low frequency range (0.1-10MHz). If interested, I can send you some excerpts.

People do complex permeability measurement at GHz. For instance, refer to:
Jacquart. Influence of the electrical resistivity of a ferromagnetic thin film on its permeability measurement performed with a permeameter. Elsevier Journal of Magnetism and Magnetic Materials 281 (2004) 82–91

Best regards

Linas


 
 Reply 
 
Changqing Lee
Changqing Lee
03:37 Apr-11-2006
Re: measuring conductivity and permeability
I have seen people use alternative current potential drop (ACPD) method for measuring the electrical conductivity and the effective magnetic permeability of ferromagnatic samples at the frequency range of several hundred Hz to 10KHz. Please google it yourself.

Eddy current testing is another option. But to determine conductivity and permeability at the same time is always hard.

----------- Start Original Message -----------
: Dear Elmar,
: you wrote
: : ..We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples...
: Maybe it's a complex permeability you want to measure?
: If yes:
: .. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?...
: Then RLC meter with some mathematics on geometry will do. We have prepared the paper on toroidal samples complex permeability measurement in low frequency range (0.1-10MHz). If interested, I can send you some excerpts.
: People do complex permeability measurement at GHz. For instance, refer to:
: Jacquart. Influence of the electrical resistivity of a ferromagnetic thin film on its permeability measurement performed with a permeameter. Elsevier Journal of Magnetism and Magnetic Materials 281 (2004) 82–91
: Best regards
: Linas
------------ End Original Message ------------




 
 Reply 
 
Jim Yukes
Consultant
Canada, Joined Aug 2005, 11

Jim Yukes

Consultant
Canada,
Joined Aug 2005
11
08:15 Apr-13-2006
Re: measuring conductivity and permeability
I checked with a Queens U Magnetics Department Grad & he suggested: There are many different ways to measure permeability depending on the material and application. For some standard methods visit www.astm.org and search for standards with key words "magnetic permeability".

For the conductivity measurement, Google search phrase "contact resistance tester".

----------- Start Original Message -----------
: Dear all,
: We want to measure the electrical conductivity and the effective magnetic permeability of ferromagnatic samples. The samples typically have a flat site a few cm across. Does anyone know a lab that could do these measurements or know a straight forward method we can set-up ourselves?
: Best regards
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Content on Demand by Eddyfi Technologies

Finding yourself in front of a screen practicing safe social distancing instead of out in the fiel
...
d? At Eddyfi Technologies, we are doing our part in helping you be better prepared for what comes next. We introduce to you Eddyfi on Demand. Fill your schedule with webinars, how-to videos, informative technical papers and our NEW addition: Eddyfi Academy. There, you will have access to FREE online courses and obtain certificates of attendance once completed in order for you to include these e-learning sessions in your log of required training hours. Join us today. Stay safe, stay Beyond Current.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window