ranjeet singh
Engineering, Asst.Manager-Condition Monitoring
TATA chemicals ltd.(fertilizer div.), India, Joined May 2006, 6

ranjeet singh

Engineering, Asst.Manager-Condition Monitoring
TATA chemicals ltd.(fertilizer div.),
India,
Joined May 2006
6
01:47 May-19-2006
Ferrite Measurement in Reformer catalyst tube material Manurite 36X

We are operating a Ammonia plant (capacity 1700 TPD) and Urea plant (capacity 2250 TPD) .

We have reformer having following details:
Thickness (msw) : 11.3 mm
Material of tube : Manuarite 36X (Cr25%,Ni 35%,Nb)
Length of tube : 13.65 Mts
No of burner : 432 ( side fired )

We have measured ferrite no.using Elcometer banana type and found that in one of the tube FN is 13.5 .
Let me know how much is allowed in such centrifugally casted tube in high temp.environment.
As per our knowlege 13.5 FN means 13.5% austinite has converted into ferrite strcuture

Awaiting your reply,

Best regards,



 
 Reply 
 

Product Spotlight

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

High-end Ultrasonic Flaw Detector with 32:128PR PAUT and 2-ch TOFD: SyncScan 2

SIUI’s newly launched SyncScan 2, is a high-end ultrasonic flaw detector with 32:128PR PAUT and
...
2-ch TOFD, which can maximize your efficiency for PA and TOFD. ● Support PA/TOFD/UT ● 32-ch PA is more suitable for inspection on extra-thick wall and high-attenuation material. ● 32-ch PA and 2-ch TOFD work simultaneously. ● Support PR mode for corrosion inspection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window