ULTRASOUND INSTITUTE
The Ultrasound Institute can develop new advanced ultrasonic measurement, imaging and NDT techniques for non-conventional applications.
423 views
Technical Discussions
Azhar Jamil
Engineering, NDT Mechanical Engineer
Pakistan, Joined Feb 2005, 3

Azhar Jamil

Engineering, NDT Mechanical Engineer
Pakistan,
Joined Feb 2005
3
04:10 Jun-03-2006
Re: Demagnetization

Dear Mr. K. Anandam

Thanks for your reply. We have a portable current flow (6K) MPI unit. I think we can use this for de-magnetization, what are your comments regarding that ... if possible explain the procedure in brief.

Regards
Azhar Jamil



 
 Reply 
 
ludovic klein
ludovic klein
01:49 Jun-07-2006
Re: Demagnetization
In fact I use some electrical cables in copper (95 mm²) and I make several turns all around the piece and I make an electrical current.
Regards
----------- Start Original Message -----------
: Dear Mr. K. Anandam
: Thanks for your reply. We have a portable current flow (6K) MPI unit. I think we can use this for de-magnetization, what are your comments regarding that ... if possible explain the procedure in brief.
: Regards
: Azhar Jamil
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window