where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Matec Instrument Companies, Inc.
Ultrasonic test instrumentation and systems for quality control inspection and production testing applications and scientific research.
3187 views
Technical Discussions
Sunny
Sunny
05:02 Jun-21-2006
UT Immersion system

Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide

Thanks


 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:25 Jun-21-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

We, Mahindra Intertrade Ltd has built many Immersion Tank systems for various Customers in India. We can supply Manipulators, Electronics, Software etc., depends on application and Customer reqts.

For further details, contact us.

Regards.

D.Simon Amallraja


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
05:19 Jun-22-2006
Re: UT Immersion system
This is the link for Midas (ex-Meccasonics people) who manufacture immersion systems in the UK:

www.midas-ndt.co.uk

----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------




 
 Reply 
 
Athanasios Anastasopoulos
Director,
Mistras Group, Greece, Joined Jan 2000, 14

Athanasios Anastasopoulos

Director,
Mistras Group,
Greece,
Joined Jan 2000
14
03:44 Jun-22-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

Have a look at the following manufacturers:

http://www.ndtautomation.com

http://www.olympusndt.com

We develope and supply analysis and evaluation s/w, UTIA, specially designed for immersion systems. For additional info please visit www.envirocoustics.gr or specifically for UTIA
http://www.envirocoustics.gr/software/utia/utia_eng.htm



 
 Reply 
 
Phil Thayer
Phil Thayer
04:44 Jun-22-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

We, NDT Automation manufacture a full range of immersion systems from small lab systemss to large industrial scanners. NDTA manufactures our own UT system cards (including GE approval for disc inspection). Please visit our web site at www.ndtautomation.com


 
 Reply 
 
Shmuel Saitowitz
Shmuel Saitowitz
05:46 Jun-22-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

ScanMaster Systems is the world's leader in the supply of ultrasonic inspection systems with over 300 installations world wide. ScanMaster has approvals from the large aerospace manufactures such as GEAE, Rolls Royce, MTU, Snecma and Pratt & Whitney. Systems are installed at customers like GE, Pratt & Whitney, Aubert Duvall/Fortech, MTU, TEI, Denel Aerospace, Boeing, Wyman Gordon, Boeing, amongst many others.

ScanMaster has local representation all over the world and service and support in all countries where installations have taken place.





 
 Reply 
 
Patrick Louviot
Patrick Louviot
08:38 Jun-23-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

You can try www.metalscan.fr
Metalscan is a UT specialist since 1985.



 
 Reply 
 
James Dolfi
Director
ford, USA, Joined Oct 1999, 8

James Dolfi

Director
ford,
USA,
Joined Oct 1999
8
05:51 Jun-23-2006
Re: UT Immersion system
----------- Start Original Message -----------
: : Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: : Thanks
: You can try www.metalscan.fr
: Metalscan is a UT specialist since 1985.
------------ End Original Message ------------


You can get more information at applied metrics.
They have made systems to check spot welds and material properties etc. Marv Fleming is the President of this company mail mmf@applied-metrics.com.

Hope this helps.



 
 Reply 
 
K S Lakshmanan
K S Lakshmanan
07:25 Jun-24-2006
Re: UT Immersion system
Dear Sir,

We would like to inform that we are the authorized / exclusive Representative of Olympus NDT for their complete range of Products in India (Panametrics NDT (U.S.A.), R/D Tech (Canada), Staveley NDT (U.S.A.) are the business units of Olympus NDT).

We had supplied many ultrasonic immersion systems in INDIA.

We request you to please let us know your requirement in detail, full address, contact phone numbers to enable us to submit our Offer.

Best Regards

K.S.Lakshmanan,

General Manager

Testing Machines Department

Blue Star Limited

No. 46, Cathedral Road

Chennai - 600 086

Direct No. 0091 44 4244 4250

Mobile No. 99400 36849

Board No. 0091 44 4244 4000

Fax No. 0091 44 4244 4190 / 0091 44 28116736

----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------




 
 Reply 
 
David LAVASTRE
David LAVASTRE
05:47 Jun-24-2006
Re: UT Immersion system
Hi Sunny,
Many manufacturers can provide UT systems qualified following GEAE specs.
With GEAE specifications, the UT systems (instrument+transducers) must be registered in a "Data For Ordering" file and you can use only transducers and instrument that are in DFOs.
Also, The "tank" must met with GEAE specs geometric requirements.
The manufacturers that are already qualified that I know are ;
Matec (USA)> http://www.matec.com/
IRT Scanmaster (Israel)> http://www.scanmaster-irt.com/
BIA (France > http://www.bia.fr/
GE Inspection Technologies (USA)>http://www.geinspectiontechnologies.com/index.html

For the instruments and transducers, and for conventional immersion UT, GEAE suppliers use ;
Harisonic transducers (now Olympus NDT) > http://www.olympusndt.com/
Megasonic IHM and TLC transducers.

I think that you can ask for DFOs to Mr Thadd Patton at thadd.patton@ae.ge.com

David



 
 Reply 
 
Tristian
Tristian
07:36 Nov-27-2006
Addison
Hello%2C+nice+site+look+


 
 Reply 
 

Product Spotlight

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window