04:31 Jun-26-2006
Inspection of concrete pillars

Can any one knows that how to found deterioration in the concrete pillar which supports steam turbine foundations.

for any queries please contact

regards



 
 Reply 
 
Herman J. Quakkelsteijn
Herman J. Quakkelsteijn
07:36 Jun-26-2006
Re: Inspection of concrete pillars
RTD developed a pulsed eddy current technique able to detect general wall loss on ferrous objects without the removal of concrete. Technique is proven on the legs of spherical tanks with up to 200 mm of concrete.

----------- Start Original Message -----------
: Can any one knows that how to found deterioration in the concrete pillar which supports steam turbine foundations.
: for any queries please contact
: regards
------------ End Original Message ------------




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:26 Jun-27-2006
Re: Inspection of concrete pillars
You may need to provide more detail about the problem to solicit a response. i.e what thickness of concrete and damage mechanism you are seeking. If the concrete pillars are simple reinforced concrete, techniques such as Impact Echo or Acoutsic Emission from Corroding Rebar may be effective. Thicker sections and foundations techniques such as Ground Penetrating radar might provide data.



 
 Reply 
 
Ernst Niederleithinger
Ernst Niederleithinger
03:42 Jun-27-2006
Re: Inspection of concrete pillars
Dear Azhel Jamir,
There are a lot of possibilities: Ultrasonics, radar, x-ray, Schmidt-hammer,....
More information (geometry, accessibility,...) is needed to select proper method.
Regards, Ernst Niederleithinger
----------- Start Original Message -----------
: Can any one knows that how to found deterioration in the concrete pillar which supports steam turbine foundations.
: for any queries please contact
: regards
------------ End Original Message ------------




 
 Reply 
 
R. O. Duesing
R. O. Duesing
03:47 Jun-27-2006
Re: Inspection of concrete pillars
----------- Start Original Message -----------
: You may need to provide more detail about the problem to solicit a response. i.e what thickness of concrete and damage mechanism you are seeking. If the concrete pillars are simple reinforced concrete, techniques such as Impact Echo or Acoutsic Emission from Corroding Rebar may be effective. Thicker sections and foundations techniques such as Ground Penetrating radar might provide data.
------------ End Original Message ------------

Acoustic Emission is an excellent method for testing composite structures, in this instance concrete reinforced columns. On pre and post stressed concrete bridges and concrete support columns; i.e. highway overpasses, stepped loading and dynamic loading is applied while being monitored with Acoustic Emission sensors. The best scenario is to monitor suspect columns/spans at the same time with known good columns/spans in a comparative test.



 
 Reply 
 

Product Spotlight

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window