Robert McMillen
Robert McMillen
01:28 Jul-10-2006
weld testing bulkhead / deck penetrations

A bulkhead penetration is basically a pipe passing through a steel ship's bulkhead. Once the pipe is welded and the weld is tested for watertightness (not for structural integrety), an electrical cable can then be passed through the penetration. Currently, two mechanics are required to test the penetration. One mechanic routes an air hose to one side while the other carries a bucket of soap suds with a brush to the other side of the bulkhead. Air is applied on one side and the other mechanic applies the soap and looks for bubbles. This is a two man operation which take a lot of time. Does anyone know of a simple (shipyard mechanic simple) means of testing a weld on one side of a bulkhead for watertight integrety (looking for holes in the welds only? The penetrations are normally 1 to 3 inches in diameter.


 
 Reply 
 
John Woollven
John Woollven
07:58 Jul-11-2006
Re: weld testing bulkhead / deck penetrations
We have successfully tested penetrations using UE Systems ultrasonic leak testing equipment. We would place an ultrasonic tone generator on one side and scan for leakage on the other side. Several penetrations can be tested at one time using this method.

We verified the process by making several mockups with pinhole leaks. Of course the testing is done prior to coating.

John

----------- Start Original Message -----------
: A bulkhead penetration is basically a pipe passing through a steel ship's bulkhead. Once the pipe is welded and the weld is tested for watertightness (not for structural integrety), an electrical cable can then be passed through the penetration. Currently, two mechanics are required to test the penetration. One mechanic routes an air hose to one side while the other carries a bucket of soap suds with a brush to the other side of the bulkhead. Air is applied on one side and the other mechanic applies the soap and looks for bubbles. This is a two man operation which take a lot of time. Does anyone know of a simple (shipyard mechanic simple) means of testing a weld on one side of a bulkhead for watertight integrety (looking for holes in the welds only? The penetrations are normally 1 to 3 inches in diameter.
------------ End Original Message ------------




 
 Reply 
 
S.Senthilkumar
S.Senthilkumar
04:31 Jul-13-2006
Re: weld testing bulkhead / deck penetrations
A bulkhead can be tested for full penetration by Ultrasonic will be more approprite. RT can tell only any volumemetric defect. Using the approprite transuducer angle it will be possible to ensure the penetration.
Good bye
S.Senthilkumar


 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
01:46 Jul-13-2006
Re: weld testing bulkhead / deck penetrations
Sonatest has just launched the 'SoundScan' system for this application. It has been proven on shipboard, aviation, military and orbital applications for leak detection.

Contact me for more information or check out our web-page

----------- Start Original Message -----------
: We have successfully tested penetrations using UE Systems ultrasonic leak testing equipment. We would place an ultrasonic tone generator on one side and scan for leakage on the other side. Several penetrations can be tested at one time using this method.
: We verified the process by making several mockups with pinhole leaks. Of course the testing is done prior to coating.
: John
: : A bulkhead penetration is basically a pipe passing through a steel ship's bulkhead. Once the pipe is welded and the weld is tested for watertightness (not for structural integrety), an electrical cable can then be passed through the penetration. Currently, two mechanics are required to test the penetration. One mechanic routes an air hose to one side while the other carries a bucket of soap suds with a brush to the other side of the bulkhead. Air is applied on one side and the other mechanic applies the soap and looks for bubbles. This is a two man operation which take a lot of time. Does anyone know of a simple (shipyard mechanic simple) means of testing a weld on one side of a bulkhead for watertight integrety (looking for holes in the welds only? The penetrations are normally 1 to 3 inches in diameter.
------------ End Original Message ------------




 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
01:47 Jul-13-2006
Re: weld testing bulkhead / deck penetrations
Sonatest has just launched the 'SoundScan' system for this application. It has been proven on shipboard, aviation, military and orbital applications for leak detection.

Contact me for more information or check out our web-page in a couple of weeks

Joe


----------- Start Original Message -----------
: We have successfully tested penetrations using UE Systems ultrasonic leak testing equipment. We would place an ultrasonic tone generator on one side and scan for leakage on the other side. Several penetrations can be tested at one time using this method.
: We verified the process by making several mockups with pinhole leaks. Of course the testing is done prior to coating.
: John
: : A bulkhead penetration is basically a pipe passing through a steel ship's bulkhead. Once the pipe is welded and the weld is tested for watertightness (not for structural integrety), an electrical cable can then be passed through the penetration. Currently, two mechanics are required to test the penetration.One mechanic routes an air hose to one side while the other carries a bucket of soap suds with a brush to the other side of the bulkhead. Air is applied on one side and the other mechanic applies the soap and looks for bubbles. This is a two man operation which take a lot of time. Does anyone know of a simple (shipyard mechanic simple) means of testing a weld on one side of a bulkhead for watertight integrety (looking for holes in the welds only? The penetrations are normally 1 to 3 inches in diameter.
------------ End Original Message ------------




 
 Reply 
 
Simon Amallraja
Simon Amallraja
08:45 Jul-14-2006
Re: weld testing bulkhead / deck penetrations
----------- Start Original Message -----------
: A bulkhead penetration is basically a pipe passing through a steel ship's bulkhead. Once the pipe is welded and the weld is tested for watertightness (not for structural integrety), an electrical cable can then be passed through the penetration. Currently, two mechanics are required to test the penetration. One mechanic routes an air hose to one side while the other carries a bucket of soap suds with a brush to the other side of the bulkhead. Air is applied on one side and the other mechanic applies the soap and looks for bubbles. This is a two man operation which take a lot of time. Does anyone know of a simple (shipyard mechanic simple) means of testing a weld on one side of a bulkhead for watertight integrety (looking for holes in the welds only? The penetrations are normally 1 to 3 inches in diameter.
------------ End Original Message ------------

Zetec has made special probes for these kind of application. Log on to www.zetec.com or mail to kevin.archer@zetec.com - product specialist will help you for this application.

Simon Amallraja.


 
 Reply 
 

Product Spotlight

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window