00:25 Aug-14-2006
Looking for robust coupling device/method for contact auto-UT inspection

Any information on auto-contact UT inspection system is appreciate.



 
 Reply 
 
Wolfgang Bisle
R & D, Project leader & Group Leader InService Inspect.
Airbus Deutschland GmbH, Germany, Joined Jul 2000, 35

Wolfgang Bisle

R & D, Project leader & Group Leader InService Inspect.
Airbus Deutschland GmbH,
Germany,
Joined Jul 2000
35
09:59 Aug-15-2006
Re: Looking for robust coupling device/method for contact auto-UT inspection
You should explain, what you mean....




 
 Reply 
 
Paul Heckman
Paul Heckman
00:00 Aug-15-2006
Re: Looking for robust coupling device/method for contact auto-UT inspection
----------- Start Original Message -----------
: Any information on auto-contact UT inspection system is appreciate.
------------ End Original Message ------------
What type of product are you looking to inspect? I have a contact in US who makes system for round product inspection in grinders.



 
 Reply 
 
Mark Potter
Mark Potter
01:00 Aug-15-2006
Re: Looking for robust coupling device/method for contact auto-UT inspection
----------- Start Original Message -----------
: Any information on auto-contact UT inspection system is appreciate.
------------ End Original Message ------------

It depends heavily on what you are inspecting:- conductive, insulating, of irregular shape etc., as well as wether you can tolerate pressures or couplant fluids on the part under test.

Mark.


 
 Reply 
 
Linxiao Yu
R & D, NDE in Oil & Gas; Energy; Manufacturing
BP, USA, Joined Aug 2006, 13

Linxiao Yu

R & D, NDE in Oil & Gas; Energy; Manufacturing
BP,
USA,
Joined Aug 2006
13
05:38 Aug-16-2006
Re: Looking for robust coupling device/method for contact auto-UT inspection
----------- Start Original Message -----------
: : Any information on auto-contact UT inspection system is appreciate.
: It depends heavily on what you are inspecting:- conductive, insulating, of irregular shape etc., as well as wether you can tolerate pressures or couplant fluids on the part under test.
: Mark.
------------ End Original Message ------------

Metal parts; flat or curved surface; pressure and couplant gel are acceptable.

thanks


 
 Reply 
 
Linxiao Yu
R & D, NDE in Oil & Gas; Energy; Manufacturing
BP, USA, Joined Aug 2006, 13

Linxiao Yu

R & D, NDE in Oil & Gas; Energy; Manufacturing
BP,
USA,
Joined Aug 2006
13
06:53 Aug-16-2006
Re: Looking for robust coupling device/method for contact auto-UT inspection
----------- Start Original Message -----------
: You should explain, what you mean....
------------ End Original Message ------------

Thank you all for your response!

I am developing an auto-inspection system using contact UT. Constant coupling of ultrasound into part is a concern. We are interested in a device (or fixture, coupling mechanism) to ensure consistent coupling. Commercially available product is highly desirable. Information on an overall system is also appreciated.

The access surfaces of the parts to be inspected can be flat, or curved (OD of cylinder).

Thank you all for your information


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
01:42 Aug-21-2006
Re: Looking for robust coupling device/method for contact auto-UT inspection
What about water perhaps with an inhibitor and a surfactant? Probe and wedge manufacturers will be able to provide you with wedges with stragetically sited drilled holes in a groove on the base of the wedge connected by bayonet-fittings to a water supply through a small bore tube. Cleanliness of the water supply is essential - it should be potable water. This is used for offshore AUT where the pipes can be still hot when the probes come into contact with the surface.

Devise some form of couplant-monitoring.


----------- Start Original Message -----------
: : You should explain, what you mean....
: Thank you all for your response!
: I am developing an auto-inspection system using contact UT. Constant coupling of ultrasound into part is a concern. We are interested in a device (or fixture, coupling mechanism) to ensure consistent coupling. Commercially available product is highly desirable. Information on an overall system is also appreciated.
: The access surfaces of the parts to be inspected can be flat, or curved (OD of cylinder).
: Thank you all for your information
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window