Coating thickness

I need to find out the thickness of a Polyurea coating being applied to foam backing. Does anybody have experience with this?

Thanks.


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
02:31 Sep-28-2006
Re: Coating thickness
We have successfully done this sort of measurement using ultrasonic thickness gages and delay line transducers. If the coating is reasonably smooth, bubble-free, and at least 0.5 mm thick, we may be able to help you. The potential limitations are rough outside surfaces or the presence of air bubbles within the coating, both of which will scatter the sound waves.

----------- Start Original Message -----------
: I need to find out the thickness of a Polyurea coating being applied to foam backing. Does anybody have experience with this?
: Thanks.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Surf-X® Array Probe

Introducing the Surf-X family of flexible Eddy Current Array (ECA) probes. Featuring unique multiple
...
coil sets and proprietary X-PROBE technology, Surf-X array probes can quickly and accurately handle a range of inspection applications, from inspecting corrosion or cracking in pipes, pressure vessels, or tanks, to assessing and sizing cracks in raised welds and friction stir welds.
>

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window