01:56 Aug-18-1999
Flash Radiography

Is flash radiography only used in laboratory applications or has it practical uses as well? From what I have seen on the net it does not appear too portable


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
04:59 Aug-18-1999
Re: Flash Radiography
: Is flash radiography only used in laboratory applications or has it practical uses as well? From what I have seen on the net it does not appear too portable

Lixi, Inc. manufactures a portable flash unit at
140KV and battery operated. If you would like to
see images and a picture of the unit, please provide
us your Email address.



 
 Reply 
 
Majed Al-Rassi
Majed Al-Rassi
02:16 Sep-02-2000
Re: Flash Radiography
: We wish to scan 8" inulated pipe line for wall thickness profile at selected zones, without removing cold insulation. Is it psssible? If so can you render the sevices? The pipe line is operated at -33°C Liq. ammonia line insulated; pipe material is killed carbon steel about 9 mm thick.

Majed Al-Rassi
Inspection Superintendent
Safco
Al-Jubail
Tel 0096633606656
Fax 0096633410147
E Mail MRassi@SAFCO.NET


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
09:38 Sep-06-2000
Flash Radiography
Lixi Profiler will meet all of the conditions outlined
in your request. Made attempt to reply to your Email
Address but the number listed was not accepting Email.


Regards,

Joe Pascenet

: : We wish to scan 8" inulated pipe line for wall thickness profile at selected zones, without removing cold insulation. Is it psssible? If so can you render the sevices? The pipe line is operated at -33°C Liq. ammonia line insulated; pipe material is killed carbon steel about 9 mm thick.

: Majed Al-Rassi
: Inspection Superintendent
: Safco
: Al-Jubail
: Tel 0096633606656
: Fax 0096633410147
: E Mail MRassi@SAFCO.NET




 
 Reply 
 
Michel Couillard
Michel Couillard
03:22 Mar-02-2001
Re: Flash Radiography (for pictures )
: : Is flash radiography only used in laboratory applications or has it practical uses as well? From what I have seen on the net it does not appear too portable

: Lixi, Inc. manufactures a portable flash unit at
: 140KV and battery operated. If you would like to
: see images and a picture of the unit, please provide
: us your Email address.




 
 Reply 
 
mathew
mathew
03:46 Jul-09-2002
Re: Flash Radiography (for pictures )
: : : Is flash radiography only used in laboratory applications or has it practical uses as well? From what I have seen on the net it does not appear too portable
.
: : Lixi, Inc. manufactures a portable flash unit at
: : 140KV and battery operated. If you would like to
: : see images and a picture of the unit, please provide
: : us your Email address.
.
1



 
 Reply 
 
Jim Knowles
Jim Knowles
00:03 Jul-09-2002
Re: Flash Radiography
: Is flash radiography only used in laboratory applications or has it practical uses as well? From what I have seen on the net it does not appear too portable

: You need to consider the application and item to be inspected.
Also look at the equipment avaialble from JME Ltd.
e-mail info@jme.co.uk
www.jme.co.uk




 
 Reply 
 

Product Spotlight

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>