Matec Instrument Companies, Inc.
Ultrasonic test instrumentation and systems for quality control inspection and production testing applications and scientific research.
850 views
Technical Discussions
Paolo
NDT Inspector,
Acciaierie Valbruna, Italy, Joined Nov 2006, 7

Paolo

NDT Inspector,
Acciaierie Valbruna,
Italy,
Joined Nov 2006
7
04:56 Mar-01-2007
ET testing for long products

Does anybody know ET standards for examination of steel long products (es. round bars)?
Thanks
Paolo


 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:19 Mar-06-2007
Re: ET testing for long products
----------- Start Original Message -----------
: Does anybody know ET standards for examination of steel long products (es. round bars)?
: Thanks
: Paolo
------------ End Original Message ------------

Contact Mr. Phil Herman Jr @ www.phtool.com and you will get the answer.

Simon


 
 Reply 
 
Debdutta Mallik
Consultant,
Malaysia, Joined Jun 2005, 37

Debdutta Mallik

Consultant,
Malaysia,
Joined Jun 2005
37
04:22 Apr-18-2007
Eddy Current Testing for long products
Dear Paolo,
There must be a standard for acceptance criteria of for eddy current testing of your product.If it is a long product then it can be done by online system. What kind of system you have.
For eddy current generally transverse or longitudinal notches are followed for calibration.starting from 0.2 and onwards depending upon the requirement of the specification.I can provide you the information regarding online surface inspection of rails.
Dont hesitate to ask if any further information required.

Best Regards,

Debdutta Mallik


 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 222

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
222
03:16 Apr-26-2007
Re: Eddy Current Testing for long products
Please see NEWT International's website. I'm sure we can help you.

----------- Start Original Message -----------
: Dear Paolo,
: There must be a standard for acceptance criteria of for eddy current testing of your product.If it is a long product then it can be done by online system. What kind of system you have.
: For eddy current generally transverse or longitudinal notches are followed for calibration.starting from 0.2 and onwards depending upon the requirement of the specification.I can provide you the information regarding online surface inspection of rails.
: Dont hesitate to ask if any further information required.
: Best Regards,
: Debdutta Mallik
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>