hello,

any pl. guide me on ut in lieu of rt,our fabrication code asme b.31.1.

also, i would like to inform you all that we welding pipe with pipe fitting i.e. pipe to elbow,tee,reducer etc. thk. between 3 mm to 70 mm.dia between 15 nb to 500 nb & over.material as,cs,ss.
thanks.


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
01:38 May-11-2007
Re: ndt
Hi (Mr) Munda

ASME B31.1 allows UT where t > 19mm. (Table 136.4). You may wish to check with ASME if B31.3 Code Case 181 (Pressure Piping) (Alternative acceptance criteria)has also been issued for B31.1. (Power Piping)

Regards

Nigel

----------- Start Original Message -----------
: hello,
: any pl. guide me on ut in lieu of rt,our fabrication code asme b.31.1.
: also, i would like to inform you all that we welding pipe with pipe fitting i.e. pipe to elbow,tee,reducer etc. thk. between 3 mm to 70 mm.dia between 15 nb to 500 nb & over.material as,cs,ss.
: thanks.
------------ End Original Message ------------




 
 Reply 
 
hassan mujadad
hassan mujadad
01:56 May-13-2007
Re: ndt
----------- Start Original Message -----------
: Hi (Mr) Munda
: ASME B31.1 allows UT where t > 19mm. (Table 136.4). You may wish to check with ASME if B31.3 Code Case 181 (Pressure Piping) (Alternative acceptance criteria)has also been issued for B31.1. (Power Piping)
: Regards
: Nigel
: : hello,
: : any pl. guide me on ut in lieu of rt,our fabrication code asme b.31.1.
: : also, i would like to inform you all that we welding pipe with pipe fitting i.e. pipe to elbow,tee,reducer etc. thk. between 3 mm to 70 mm.dia between 15 nb to 500 nb & over.material as,cs,ss.
: : thanks.
------------ End Original Message ------------

for this purpose you will use asme Sec V or table given in ASME B 31.3 table# 136.4 page # 97
this will guide you throughout thichness wise And DIA wise
thanks
Regard,s
Hassan Mujadad


 
 Reply 
 

Product Spotlight

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window