resin content monitoring in prepregs

Hi all,

We develop industrial low energy X-ray method and apparatus for monitoring of resin content in prepregs during production. Can anybody give us his thoughts about this method or show us a link where a X-ray method is used at presence in prepregs manufacturing?

Any thoughts will be greatly appreciated

Sincerelly,
Dr. Nikitin




 
 Reply 
 
John Brunk
Engineering, NDT Level III
Self employed, part-time, USA, Joined Oct 1999, 161

John Brunk

Engineering, NDT Level III
Self employed, part-time,
USA,
Joined Oct 1999
161
00:33 Jun-10-2007
Re: resin content monitoring in prepregs
----------- Start Original Message -----------
: Hi all,
: We develop industrial low energy X-ray method and apparatus for monitoring of resin content in prepregs during production. Can anybody give us his thoughts about this method or show us a link where a X-ray method is used at presence in prepregs manufacturing?
: Any thoughts will be greatly appreciated
: Sincerelly,
: Dr. Nikitin
------------ End Original Message ------------
You should take a careful look at the attenuation coefficients of the materials involved. X-ray may not be the best method for distinguishing graphite from the resin. Looking for actual voids is a different matter. Air-transmission ultrasound would be worth consideration.

John Brunk


 
 Reply 
 

Product Spotlight

Magnetic X-Ray Pipeline Crawler

Zhong Yi brand pipeline crawler is magnetic/micro-video controlled crawler with DC X ray unit inst
...
alled for checking welding of pipeline. Move steadily inside the pipeline 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometers and provide the efficient inspection of the pipeline.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window