DIKDIK
DIKDIK
05:55 Oct-01-2007
OES Portable

We plan to buy an alloy analyzer. We consider about OES portable. Did anyone has experience about this kind of instrument ? Which type/model/manufacturer is the best instrument ?

thanks
dik2


 
 Reply 
 
Rohit Bafna
,
TCR Engineering Services, India, Joined Sep 2007, 18

Rohit Bafna

,
TCR Engineering Services,
India,
Joined Sep 2007
18
07:25 Oct-01-2007
Re: OES Portable
At TCR Engineering Services, we routinely provide PMI services using both XRF and OES Spectrometers all over the world. We use Arcmet 8000 for the portable OES.

I highly recommend this equippment




 
 Reply 
 
Dang Dinh Tuan
Sales, - -
Automation System Integration & Technology Transfer, Vietnam, Joined Nov 2007, 3

Dang Dinh Tuan

Sales, - -
Automation System Integration & Technology Transfer,
Vietnam,
Joined Nov 2007
3
01:02 Oct-01-2007
Re: OES Portable
Hello,

PMI Master Pro
from WAS (www.was-ag.com) is the best portable OES.

Good luck!

----------- Start Original Message -----------
: We plan to buy an alloy analyzer. We consider about OES portable. Did anyone has experience about this kind of instrument ? Which type/model/manufacturer is the best instrument ?
: thanks
: dik2
------------ End Original Message ------------




 
 Reply 
 
kATHY f
kATHY f
00:12 Oct-02-2007
Re: OES Portable
----------- Start Original Message -----------
: Hello,
: PMI Master Pro
: from WAS (www.was-ag.com) is the best portable OES.
: Good luck!
: : We plan to buy an alloy analyzer. We consider about OES portable. Did anyone has experience about this kind of instrument ? Which type/model/manufacturer is the best instrument ?
: : thanks
: : dik2
------------ End Original Message ------------
I NEED A USERS MANUAL FOR THE OES PORTABLE 8000





 
 Reply 
 
LOO LT
LOO LT
01:04 Oct-03-2007
Re: OES Portable
Dear Sir,

We are the sole agents for the popular WAS PMI specialist for Southeast Asia market. Please provide us your full contact detail, so that I can get my engineer to get in touch with you.

Best regard,

Loo
+6016 322 8368

----------- Start Original Message -----------
: We plan to buy an alloy analyzer. We consider about OES portable. Did anyone has experience about this kind of instrument ? Which type/model/manufacturer is the best instrument ?
: thanks
: dik2
------------ End Original Message ------------




 
 Reply 
 
DIKDIK
DIKDIK
00:00 Oct-06-2007
Re: OES Portable
You can contact me at :
dikdiky@pusri.co.id

thanks

----------- Start Original Message -----------
: Dear Sir,
: We are the sole agents for the popular WAS PMI specialist for Southeast Asia market. Please provide us your full contact detail, so that I can get my engineer to get in touch with you.
: Best regard,
: Loo
: +6016 322 8368
: : We plan to buy an alloy analyzer. We consider about OES portable. Did anyone has experience about this kind of instrument ? Which type/model/manufacturer is the best instrument ?
: : thanks
: : dik2
------------ End Original Message ------------




 
 Reply 
 
Amit Bafna
Amit Bafna
04:25 Oct-06-2007
Re: OES Portable
Arcmet 8000 from Metorex can also be a good option for OES portable.
----------- Start Original Message -----------
: We plan to buy an alloy analyzer. We consider about OES portable. Did anyone has experience about this kind of instrument ? Which type/model/manufacturer is the best instrument ?
: thanks
: dik2
------------ End Original Message ------------




 
 Reply 
 
Dave
Dave
01:39 Nov-10-2007
Re: OES Portable
----------- Start Original Message -----------
: Arcmet 8000 from Metorex can also be a good option for OES portable.
: : We plan to buy an alloy analyzer. We consider about OES portable. Did anyone has experience about this kind of instrument ? Which type/model/manufacturer is the best instrument ?
: : thanks
: : dik2
------------ End Original Message ------------

Porbable is not really portable when dealing with OES.

Take a look at NITON XRF!


 
 Reply 
 

Product Spotlight

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window