WPS

Dear All,

Please help me ? Code/ Standard: ASME IX/ ASME B31.3

If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?

Many thanks for your support.



 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
02:15 Dec-28-2007
Re: WPS
Dear Du Xuan Binh

Is your English good enough to read the Codes (it certainly seems quite good from your post) or is there a Vietnamese translation of the Codes? From your profile you work for BP they must have a good technical library.

Access the quoted code and read it - in the long run it will serve you better than being given answers from sources you have no knowledge of. This is an NDT forum, members cannot be expected to have sound knowledge of Code welding rules. AWS has a website with a technical forum or you can try Eng Tips.

---------- Start Original Message -----------
: Dear All,
: Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: Many thanks for your support.
------------ End Original Message ------------




 
 Reply 
 
G.Madhesan
Consultant, Welding ýnspector/QAQC inspector
CHENNAI UNIVERSITY, Turkey, Joined Nov 2004, 10

G.Madhesan

Consultant, Welding ýnspector/QAQC inspector
CHENNAI UNIVERSITY,
Turkey,
Joined Nov 2004
10
04:54 Dec-29-2007
Re: WPS
A333 Gr.6 material is different from API 5L X60 material.At any temperature it will not be qualified to each other.


----------- Start Original Message -----------
: Dear Du Xuan Binh
: Is your English good enough to read the Codes (it certainly seems quite good from your post) or is there a Vietnamese translation of the Codes? From your profile you work for BP they must have a good technical library.
: Access the quoted code and read it - in the long run it will serve you better than being given answers from sources you have no knowledge of. This is an NDT forum, members cannot be expected to have sound knowledge of Code welding rules. AWS has a website with a technical forum or you can try Eng Tips.
: ---------- Start Original Message -----------
: : Dear All,
: : Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: : If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: : Many thanks for your support.
------------ End Original Message------------




 
 Reply 
 
Welding Guy
Welding Guy
04:01 Dec-30-2007
Re: WPS
----------- Start Original Message -----------
: Dear All,
: Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: Many thanks for your support.
------------ End Original Message ------------

I believe this has already been posted on the AWS forum and answered.
I believe this was the answer you got:

A333, Gr 6 is P1, Gr. 1, and API 5L X60 is P1, Gr. 2.

Since you mention CVN's the answer is "no" A333, Gr. 6 does not qualify API 5L, X60, see QW-403.5; supplementary essential variable.


 
 Reply 
 
victorsteel
victorsteel
19:37 Aug-25-2014
Re: WPS
In Reply to Welding Guy at 04:01 Dec-30-2007 .

u will get all Standard and grades of api 5lx60 on http://www.api5lx60.com/

 
 Reply 
 

Product Spotlight

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window