07:21 Feb-21-2008
AWS D1.1 PT/MT acceptance limit

AWS D1.1 does not specify the acceptance critiera for PT/MT, just one sentence says refer to table 6.1 which is visual inspection acceptance critiera. If a porosity(non piping porosity) was found in Cyclically Loaded Nontubular Connections, How to evaluate it? Can some one explain the PT/MT acceptance critiera?

Thanks!

Eric Chen


 
 Reply 
 
chris s
chris s
07:16 Feb-21-2008
Re: AWS D1.1 PT/MT acceptance limit
----------- Start Original Message -----------
: AWS D1.1 does not specify the acceptance critiera for PT/MT, just one sentence says refer to table 6.1 which is visual inspection acceptance critiera. If a porosity(non piping porosity) was found in Cyclically Loaded Nontubular Connections, How to evaluate it? Can some one explain the PT/MT acceptance critiera?
: Thanks!
: Eric Chen
------------ End Original Message ------------

eric,
what you will need to do is apply the limits in table 6.1 as your acceptance criteria. look in the commentary at c-6.10 note that you do not read bleed out. only the size of the discontinuity.



 
 Reply 
 
DEEPAK SAXENA
DEEPAK SAXENA
09:59 May-31-2008
Re: AWS D1.1 PT/MT acceptance limit
please provide visual acceptance criteria for porosity in TIG welding


 
 Reply 
 
mustafa GONULAL
Engineering,
CIMTAS / ENKA, Turkey, Joined Jun 2008, 8

mustafa GONULAL

Engineering,
CIMTAS / ENKA,
Turkey,
Joined Jun 2008
8
05:26 Jun-04-2008
Re: AWS D1.1 PT/MT acceptance limit
----------- Start Original Message -----------
: please provide visual acceptance criteria for porosity in TIG welding
------------ End Original Message ------------

Aceeptance Limit for PT/MT in AWS is defined as
CJP Groove welds in butt joints transverse to the direction of computes tensile stress shall have no visible piping porosity.
For all other groove welds and fillet welds, the sum of visible piping porosity 1mm or greater in dia. shall not exceed 10mm in any linear inch of weld and shall not exceed 20mm in any 12in. length of weld.


 
 Reply 
 
mike
mike
01:32 Aug-23-2014
Re: AWS D1.1 PT/MT acceptance limit
In Reply to chris s at 07:16 Feb-21-2008 .

AWS c-6.10 only refers to clause 6.14.4 for MT test which is very general. It basically ask for app the acceptance criteria that are in Section 6, part C, whichever is applicable. Can any one elaborate what "whichever applicable" mean? In section 6, partc there are requirements for UT and RT. Should one is applicable, ut or rt?

thanks,

 
 Reply 
 
mike
mike
01:47 Aug-23-2014
Re: AWS D1.1 PT/MT acceptance limit
In Reply to mike at 01:32 Aug-23-2014 .

AWS c-6.10 only refers to clause 6.14.4 for MT test which is very general. It basically says " acceptance shall be in conformance with Section6, part C, of this code, whichever is applicable". Can any one elaborate what "whichever applicable" mean? In section 6, part C there are only requirements for UT and RT tests. which one is applicable, UT or RT?
I assume RT, any comment?

thanks,

 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window