CHIME

all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated


 
 Reply 
 
bob sudharmn
Engineering, Reliability and Integrity Eng
Shell Malaysia Trading, Malaysia, Joined Jan 2008, 54

bob sudharmn

Engineering, Reliability and Integrity Eng
Shell Malaysia Trading,
Malaysia,
Joined Jan 2008
54
01:55 Jun-09-2008
Re: CHIME
There is an article on this subject. Refer attached link

http://www.ndt.net/article/ecndt98/chemical/103/103.htm


----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
03:53 Jun-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.

As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.



 
 Reply 
 
mj
mj
08:43 Jun-10-2008
Re: CHIME
Dear Mr. John,
Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?


----------- Start Original Message -----------
: : all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
: CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.
: As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.
------------ End Original Message ------------




 
 Reply 
 
Mark Nel
Mark Nel
03:14 Jun-10-2008
Re: CHIME
Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
----------- Start Original Message -----------
: Dear Mr. John,
: Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?



 
 Reply 
 
Charlie Lawther
Charlie Lawther
02:24 Jun-12-2008
Re: CHIME
CHIME is manufactured by ESR (Was AEA Technology) They could provide you with equipment and a license to use CHIME.

3 companies currently have a license to use this equipment.
----------- Start Original Message -----------
: Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
: : Dear Mr. John,
: : Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?
------------ End Original Message ------------




 
 Reply 
 
RT. Jeyakumar
RT. Jeyakumar
07:59 Jul-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

Good day MJ,

Olympus (RD Tech, Canada) is manufacturing equipment with CHIME software. It is user friendly too. It is no other than Olympus multi scan equipment with TOFD, CHIME, Eddy Current (Surface scanning), etc. Hope you're MJ of Malaysia. If so, contact Olympus Singapore. They can help you

Regards,

RT. Jeyakumar


 
 Reply 
 

Product Spotlight

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

SONOAIR - air-coupled Phased Array Ultrasonic Inspection System

For highly attenuating materials, the performance of the system is critical. The ultrasonic sensors,
...
the scanning area and the system settings should be flexibly adapted to the test task and the material. These high expectations are met with the new and modular testing system SONOAIR. With the world’s first air-coupled phased-array UT inspection system SONOAIR we developed a technology that works with up to 4 transmitter and receiver channels with freely configurable square wave burst transmitters as wells as low noise receiving amplifiers.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window