Jack Son
09:31 Jul-14-2008
want to ask something in UT-phased array

1. For acceptance/ reject the welds, are we
i)comparing the amplitude of a surface notch (code requirement)
or
ii)measuring the depth of root penetration.

2.Cause of insufficient root penetrant.
i)root Gap?
ii)Weld current?
iii)welding speed?
iv)or other reason




 
 Reply 
 
tj
tj
01:04 Jul-15-2008
Re: want to ask something in UT-phased array
----------- Start Original Message -----------
: 1. For acceptance/ reject the welds, are we
: i)comparing the amplitude of a surface notch (code requirement)
: or
: ii)measuring the depth of root penetration.
: 2.Cause of insufficient root penetrant.
: i)root Gap?
: ii)Weld current?
: iii)welding speed?
: iv)or other reason
------------ End Original Message ------------

Hi,
You should consult the spec for calibration requirements. The incomplete penetration is most likely due to insufficient current, however, torch angle and travel speed can play a definite role in your problem.


 
 Reply 
 

Product Spotlight

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window