coercive force

is the coercive force depend on the shape ? Provided two samples are made of the same material but different shape, you measure their coercive force could you end up with different results ?



 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 893

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
893
07:24 Sep-05-2008
Re: coercive force
In one word, YES! The lower the L/D Ratio (Length to Diameter), greater is the Coercive Force required to demagnetise the item. But shape is not the only factor. You also have to take into account such properties as heat treatment and alloying.

Cheerio's
Michel

----------- Start Original Message -----------
: is the coercive force depend on the shape ? Provided two samples are made of the same material but different shape, you measure their coercive force could you end up with different results ?
------------ End Original Message ------------




 
 Reply 
 
Catalin Mandache
Catalin Mandache
06:03 Sep-08-2008
Re: coercive force
The coercive force depends on so many micro structural factors that is very unlikely to have the same values for two identically shaped and alloyed samples.

----------- Start Original Message -----------
: is the coercive force depend on the shape ? Provided two samples are made of the same material but different shape, you measure their coercive force could you end up with different results ?
------------ End Original Message ------------




 
 Reply 
 
David Mackintosh
Engineering,
Acuren Group Inc., Canada, Joined Feb 2011, 85

David Mackintosh

Engineering,
Acuren Group Inc.,
Canada,
Joined Feb 2011
85
09:36 Sep-23-2008
Re: coercive force
----------- Start Original Message -----------
: is the coercive force depend on the shape ? Provided two samples are made of the same material but different shape, you measure their coercive force could you end up with different results ?
------------ End Original Message ------------

The coercive force, Hc, is the applied field required to demagnetize a material after saturation. It is a material property. (See for example http://www.ndt-ed.org/EducationResources/CommunityCollege/MagParticle/Physics/HysteresisLoop.htm and http://en.wikipedia.org/wiki/Coercive_force.) The magnetic H-field required to demagnetize a specific object depends on the material properties, the shape of the object, and the method of applying the field, among other things. Hc for the material and the demagnetizing force required for a specific object are related, but it is not always easy to calculate one from the other.

David



 
 Reply 
 

Product Spotlight

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window