Remaining life and replica

Is it true that Replica result can calculate remaining life of material? some guy told me that they only do replica test and they will know the life time remaining of pipe,vessel,tank!??





 
 Reply 
 
Ananthan
Consultant,
RAA Tech Solutions, India, Joined Jun 2000, 36

Ananthan

Consultant,
RAA Tech Solutions,
India,
Joined Jun 2000
36
03:35 Sep-01-2005
Re: Remaining life and replica
----------- Start Original Message -----------
: Is it true that Replica result can calculate remaining life of material? some guy told me that they only do replica test and they will know the life time remaining of pipe,vessel,tank!??
------------ End Original Message ------------

Replica tells yopu the present condition of the material. By estimating the creep cavities one can estimate the remaining life or at least the next required inspection schedule.

S S Ananthan


 
 Reply 
 

Product Spotlight

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window