Re: Coating thickness Gauge
: : Did anybody knows the equipment which can measure coating thickness on the plastic substrate?
: : Thickness of coating is 1micron to 500 micron.
: : Diameter of target is approximately 5mm(W) x 5mm(H) x 5mm(D).
I suppose that can do:
Thorsten Staedler

Fraunhofer Institut
Schicht- und Oberflächentechnik
Bienroder Weg 54E
D-38108 Braunschweig

Tel.: +49 (0)531 - 2155 - 664
Fax: +49 (0)531 - 2155 - 900

email: staedler@ist.fhg.de
with our help (concern interpretation of test result)





 
 Reply 
 
Micheal Park
R & D
Worltech R&D Center, South Korea, Joined Oct 1999, 5

Micheal Park

R & D
Worltech R&D Center,
South Korea,
Joined Oct 1999
5
08:37 Jan-04-2001
Coating thickness Gauge

Did anybody knows the equipment which can measure coating thickness on the plastic substrate?
Thickness of coating is 1micron to 500 micron.
Diameter of target is approximately 5mm(W) x 5mm(H) x 5mm(D).
Thank you!


 
 Reply 
 
Massimo Carminati
Massimo Carminati
09:11 Jan-04-2001
Re: Coating thickness Gauge
: Did anybody knows the equipment which can measure coating thickness on the plastic substrate?
: Thickness of coating is 1micron to 500 micron.
: Diameter of target is approximately 5mm(W) x 5mm(H) x 5mm(D).
: Thank you!

Try to contact your local Krautkramer agent. They have instruments (name CTM10 and CTM20, but it was three years ago).




 
 Reply 
 
dena_ahmed22
dena_ahmed22
03:55 Apr-19-2001
Re: Coating thickness Gauge
hi i want write to me information about "thickness gauge tist"


 
 Reply 
 

Product Spotlight

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window