01:05 Jan-08-2001
reference film for digitidation

Hello,

I am interested in procuring a reference film for digitising systems as per ASME Sec V - Article 2 - VI - A - 230. Can some one please help in locating a supplier for the same.
Thank You

S S Ananthan



 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
01:33 Jan-08-2001
Re: reference film for digitidation
Dear Mr. Ananthan,

You may purchase the Reference Radiograh at the EPRI NDE Center (Mr. Kim Kietzman) at (704) 547-6100 (USA).

My company, Digital Imaging Services (DIS) performs the radiographic film digitization.

Also, we conduct the 40 hours of Advanced Digital Radiography Training per the ASME Code.

DIS is located in Birmingahm, Alabama.

Sincerely,

J. Mark Davis
(205) 663-7006


: Hello,

: I am interested in procuring a reference film for digitising systems as per ASME Sec V - Article 2 - VI - A - 230. Can some one please help in locating a supplier for the same.
: Thank You

: S S Ananthan




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
05:24 Jan-10-2001
Re: reference film for digitidation
You should try AGFA NDT systems as they have a large Digital Divison now, BAM germany may also be able to help as may Fuji NDT Systems.

Regards

John O'Brien



 
 Reply 
 

Product Spotlight

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window