Gowri santhosh palika
NDT Inspector,
Royscan engineering pte ltd, Singapore, Joined May 2008, 52

Gowri santhosh palika

NDT Inspector,
Royscan engineering pte ltd,
Singapore,
Joined May 2008
52
18:05 Apr-11-2009
T K Y joints

hi

what are the main things i have to consider when i do the UT on T K Y weld joints mainly leg pipe to pipe.

 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
21:50 Apr-12-2009
Re: T K Y joints
In Reply to Gowri santhosh palika at 18:05 Apr-11-2009 (Opening).

What code or standard are you examining to and how is the accept/reject criteria established matched with understanding where the sound is actually going is a good place to start. API RP 2X has a good methodology to the examination of structural connections so I would study that. If you are new to this a well built mock up to practice on is essential.

 
 Reply 
 
R Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

R Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
04:31 Apr-13-2009
Re: T K Y joints
In Reply to John O'Brien at 21:50 Apr-12-2009 .

Another excellent source of criteria and UT guidance is AWS D1.1 Both D1.1 and RP 2X are available online from http://store.ihs.com

 
 Reply 
 
hendro harner
hendro harner
19:54 Aug-17-2011
Re: T K Y joints
In Reply to Gowri santhosh palika at 18:05 Apr-11-2009 (Opening).

to leg pipe to pipe only use class x to accepten criteria

 
 Reply 
 

Product Spotlight

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window