what's this film of rt looks like?



Pipeline 273*7mm

 
 Reply 
 
anjafo79
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo79

NDT Inspector
Norway,
Joined Aug 2009
204
11:42 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

looks like suck back on the root to me.

 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
17:31 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

Looks the same to me as well

 
 Reply 
 
anjafo79
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo79

NDT Inspector
Norway,
Joined Aug 2009
204
18:54 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to Phil at 17:31 Jan-22-2010 .

looks acceptable to me as well with out cross checking wall thickness and accept criteria.

not darker than parent material either i guess

 
 Reply 
 
BILL KIESEL
BILL KIESEL
21:15 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

looks like local negative reinforcement at the weld root, possable stress riser due to sharp appearance, definite failure point for this weld under extreme stress.

 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
23:04 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

What is this pipeline for, what is flowing through it ?

Also which specification are you working to ?

As this will determine whether or not it is acceptable, as we know the size and wt.

 
 Reply 
 
Collin Maloney
NDT Inspector, - Plant Inspector
Applus RTD, Australia, Joined Nov 2000, 147

Collin Maloney

NDT Inspector, - Plant Inspector
Applus RTD,
Australia,
Joined Nov 2000
147
05:21 Jan-23-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

look suspiciously like a burn through given that the profile of the root bead changes from thin to wide either side of the discontinuity.
I would like to know the welding technique used i.e. stove pipe. The cap weave looks typical of a stove technique. What was the o'clock position?

 
 Reply 
 

Product Spotlight

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

On Demand Webinar: Improve the Efficiency and Accuracy of Inspection Scanning

On-demand webinar on scanning technology that helps improve the efficiency and accuracy of ultrasoni
...
c inspections in oil and gas, aerospace, manufacturing and other industrial applications. The webinar features a scanning solution for multiple inspection environments, including flat and curved specimens, magnetic and nonmagnetic surfaces and raster scanning over long distances. View it today.
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window