Moisture % in wood chips

Dear Coleagues,

I need your advice on Moisture % in wood chips measurement.
Best case would be the ready device, but any ideas would be great too.
The moisture has to be measured at dryer income and outlet.
Chips are transported by conveyor belt.
The relative humidity is about 1-3%, we would like to keep it within 1.2-1.8%

Sincerely,

Linas



 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
05:15 May-15-2002
Re: Moisture % in wood chips
: Dear Coleagues,
.
: I need your advice on Moisture % in wood chips measurement.
: Best case would be the ready device, but any ideas would be great too.
: The moisture has to be measured at dryer income and outlet.
: Chips are transported by conveyor belt.
: The relative humidity is about 1-3%, we would like to keep it within 1.2-1.8%
.
: Sincerely,
.
: Linas

Dear Sir,

If you are drying the wood chips and it is your intention to measure the moisture in the drying medium, inlet and outlet, then yes it can be done.

Please contact Panametrics PCI Division.

www.panametrics.com

http://www.panametrics.com/div_pci/pages/products/abhumidity/index.shtml

Best Regards,

David Hermanutz
Panametrics NDT Melbourne



 
 Reply 
 

Product Spotlight

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window