1204 views
Technical Discussions
Tina Wilhelm
Engineering, Research Assistant
Institute for Concrete Structures, Germany, Joined Oct 2001, 1

Tina Wilhelm

Engineering, Research Assistant
Institute for Concrete Structures,
Germany,
Joined Oct 2001
1
05:37 Jul-04-2002
ultrasonic attenuation in concrete

What kind of pulse signal and analysis makes most sense for measurements of ultrasonic attenuation in concrete in the the case of longitudinal waves and ultrasonic transmission?
Who made som experience with different results for different signals and their analysis?



 
 Reply 
 
Christian Grosse
Teacher,
Technische Universität München, Germany, Joined Nov 2000, 11

Christian Grosse

Teacher,
Technische Universität München,
Germany,
Joined Nov 2000
11
07:29 Jul-05-2002
Re: ultrasonic attenuation in concrete
: What kind of pulse signal and analysis makes most sense for measurements of ultrasonic attenuation in concrete in the the case of longitudinal waves and ultrasonic transmission?
: Who made som experience with different results for different signals and their analysis?
:
.
Dear Mrs. Wilhelm, there are numerous papers about that issue as well as some measurements from different authors, e.g.:
Berthelot, J.M.; Ben Souda, M.;Robert, J.L.: "Study of wave attenuation in concrete", J. Mater. Res. 8, 1993, Nr.9, S. 2344-2353
Landis, E.N., Sha, S.P.: " Frequency-based dependent stress wave attenuation in cement based materials", J. Eng. Mech., 121, 1995, S.737-743

More recent measurements are from Koeppel (ETH, Zuerich) and Nahrath (RWTH Aachen).
Some own results I can send you directly and not through this board.
Regards, Christian



 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window