Juan Carlos Pinzon
Juan Carlos Pinzon
05:25 Jan-24-2003
standard AMS-STD-2154

I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.

Question: Is MIL-STD-2154 still active or has it been canceled?



 
 Reply 
 
Russell Austin
Russell Austin
00:08 Jan-24-2003
Re: standard AMS-STD-2154
It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.

: I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
.
: Question: Is MIL-STD-2154 still active or has it been canceled?
.



 
 Reply 
 
juan carlos pinzon
juan carlos pinzon
01:17 Jan-29-2003
Re: standard AMS-STD-2154
: It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
.
: : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: .
: : Question: Is MIL-STD-2154 still active or has it been canceled?
: .
.
Thanks Mr Austin, I interested in a copy of the standard. Unfortenately my e-mail has not enough memory to receive the file. However in some days I will tell you a new e-mail address.



 
 Reply 
 
Dr. S.M.Kulkarni
Director, VPS's COLLEGE OF ENGINEERING and TECHNOLOGY, LONAVALA
VPS's COLLEGE OF ENGINEERING and TECHNOLOGY, LONAVALA, India, Joined Oct 2002, 5

Dr. S.M.Kulkarni

Director, VPS's COLLEGE OF ENGINEERING and TECHNOLOGY, LONAVALA
VPS's COLLEGE OF ENGINEERING and TECHNOLOGY, LONAVALA,
India,
Joined Oct 2002
5
09:22 Jan-31-2003
Re: standard AMS-STD-2154
: It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
.
: : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: .
: : Question: Is MIL-STD-2154 still active or has it been canceled?
: .
.
=============
Please send me the AMS-STD-2154.
Regards
SMKulkarni


 
 Reply 
 
DOC
DOC
00:53 Mar-26-2003
Re: standard AMS-STD-2154
: It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
.
: : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: .
: : Question: Is MIL-STD-2154 still active or has it been canceled?
: .
.

Can you please send me the AMS-STD-2154 ?

bests regards



 
 Reply 
 
J.S.JOE
Sales
South Korea, Joined Sep 2002, 9

J.S.JOE

Sales
South Korea,
Joined Sep 2002
9
06:28 Mar-28-2003
Re: standard AMS-STD-2154
We are very thank you if we can receive Standard AMS-STD-2154.

best regards
J.S.JOE

: : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: .
: : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : .
: : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : .
: .
.
: Can you please send me the AMS-STD-2154 ?
.
: bests regards
.



 
 Reply 
 
Elmar Wurch Filho
Elmar Wurch Filho
04:38 Jul-17-2003
Re: standard AMS-STD-2154
I am also interested in the MIL-STD-2154.
I need to compare it to ASTM B548-90.
Please send .PDF
(elmar@recrusul.com.br - limited to 2MB files)
(elmarw@netu.unisinos.br - limited to 5MB)

Thanks. Best Regards,
Elmar Wurch Filho

: : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: .
: : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : .
: : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : .
: .
.
: Can you please send me the AMS-STD-2154 ?
.
: bests regards
.



 
 Reply 
 
Charlie Sellers
Charlie Sellers
05:57 Oct-09-2003
Re: standard AMS-STD-2154
I could use a copy of this - I am trying to determine what lower limit of defect size it can detect (depends on material I presume - if the frequency is fixed). Thanks! csellers@mqii.com


----------- Start Original Message -----------
: : : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: : .
: : : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : : .
: : : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : : .
: : .
: .
: : Can you please send me the AMS-STD-2154 ?
: .
: : bests regards
: .Please send me the AMS-STD-2154
: Thank you very much
------------ End Original Message ------------




 
 Reply 
 
Alexandre Garcia Alcaraz
Alexandre Garcia Alcaraz
00:34 Oct-30-2003
Re: standard AMS-STD-2154
Can anybody send me the file containing SAE AMS STD 2154?

It´s very URGENT!


 
 Reply 
 
Brus Jiøí
Brus Jiøí
03:08 Nov-13-2003
AMS-STD-2154
Dear freinds,
I am just looking for standard AMS STD 2154 and I
found your discussion, can you send me, please, also
this standard by e-meil ?
Thank very much for your help.


----------- Start Original Message -----------
: : : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: : .
: : : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : : .
: : : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : : .
: : .
: .
: : Can you please send me the AMS-STD-2154 ?
: .
: : bests regards
: .Please send me the AMS-STD-2154
: Thank you very much
------------ End Original Message ------------




 
 Reply 
 
Roy Delgatty
Roy Delgatty
01:03 Mar-03-2004
Re: AMS-STD-2154
I am reviewing a procedure from Bjorneborg AB and they have referenced AMS-STD-2154, Mar 1998 Class A. Could any of you folks send a copy of this standard. Thank you very much.


 
 Reply 
 
neil
neil
03:02 Mar-23-2004
Re: standard AMS-STD-2154
Hi there, was wondering if u had copy of AMS 2154 as i am in big need of a copy.

Could you email me one?

If Poss,

cheers neil


 
 Reply 
 
Leila Mello
Leila Mello
00:48 Apr-29-2004
Re: standard AMS-STD-2154
I also do need the standard AMS-STD-2154. Can you send me a copy. My e-mail is leilmello_vtc@uol.com.br.


:It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
.
: : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: .
: : Question: Is MIL-STD-2154 still active or has it been canceled?
: .
.



 
 Reply 
 
Robert Charette
Robert Charette
06:34 Oct-19-2004
Re: standard AMS-STD-2154
: : A Supplyer of miine has submitted an NDE report showing that some bar material was UT examined to AMS-STD-2154. I am not aware of the requirements or acceptance levels of this standard.
Would you please send me a copy of this standard.

Thanks for your help.

Regards
R. Charette




 
 Reply 
 
roc
roc
01:45 Nov-02-2004
Re: standard AMS-STD-2154
could you plz send the pdf about ams-std-2154 to me.
thx//bow

: It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
.
: : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: .
: : Question: Is MIL-STD-2154 still active or has it been canceled?
: .
.



 
 Reply 
 
John E. Simpson
John E. Simpson
08:19 Nov-17-2004
Re: standard AMS-STD-2154
What is the latest revision date??
If it is after March 1998, could you please email me a copy of the latest??
My email address is jsimpson@haynesintl.com

: It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
.
: : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: .
: : Question: Is MIL-STD-2154 still active or has it been canceled?
: .
.



 
 Reply 
 
Astley Scott
Astley Scott
03:57 Feb-24-2005
Re: standard AMS-STD-2154
----------- Start Original Message -----------
: : : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: : .
: : : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : : .
: : : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : : .
: .
: : Can you please send me the AMS-STD-2154 ?
: .
: : bests regards
: .
------------ End Original Message ------------

Could you please send me a copy of the AMS-STD-2154 ?


 
 Reply 
 
Tom Morey
Tom Morey
00:30 Feb-24-2005
Re: standard AMS-STD-2154
I am also in need of a copy of AMS 2154, please e-mail. Thank you


 
 Reply 
 
Jorge Londono
Jorge Londono
01:47 Apr-25-2005
Re: standard AMS-STD-2154
May I have a copy of this standard??

I will appreciate it

Thanks.

: : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: .
: : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : .
: : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : .
: .
.
: Can you please send me the AMS-STD-2154 ?
.
: bests regards
.



 
 Reply 
 
Nathan
Nathan
09:08 Jul-08-2005
Re: standard AMS-STD-2154
Would you please send the pdf about ams-std-2154 to me.
--Greatly appreciated.

: : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: .
: : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : .
: : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : .
: .
------------ End Original Message ------------




 
 Reply 
 
Karen Upfold
Karen Upfold
03:27 Nov-17-2005
Re: standard AMS-STD-2154
Can you please e-mail me PDF for this spec

----------- Start Original Message -----------
: : : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: : .
: : : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : : .
: : Do you also have mil-std 2154, if so can you send that to.
: : .
: .: bests regards
: .
------------ End Original Message ------------





 
 Reply 
 
Jamz
Engineering
Olympus NDT, Canada, Joined Nov 2003, 2

Jamz

Engineering
Olympus NDT,
Canada,
Joined Nov 2003
2
05:56 Jan-23-2006
Re: standard AMS-STD-2154
May I have a copy of this standard?

I will appreciate it

Regards.


----------- Start Original Message -----------
: : : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: : .
: : : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : : .
: : Do you also have mil-std 2154, if so can you send that to.
: : .
: .: bests regards
: .
------------ End Original Message ------------




 
 Reply 
 
Nathan
Nathan
01:42 Aug-21-2006
Re: standard AMS-STD-2154
Will someone email me a copy of AMS STD 2154, please?


 
 Reply 
 
jason baran
jason baran
03:58 Nov-10-2006
Re: standard AMS-STD-2154
Does anyone have this spec that they can email me? Thanks.

----------- Start Original Message -----------
: May I have a copy of this standard??
: I will appreciate it
: Thanks.
: : : It is active, 44 pages, and I can send you a pdf of it (~5 MB) if you need it and supply an e-mail address.
: : .
: : : : I am aware that UT Standard SAE AMS-STD-2154 was developed to supersede MIL-STD-2154.
: : : .
: : : : Question: Is MIL-STD-2154 still active or has it been canceled?
: : : .
: : .
: .
: : Can you please send me the AMS-STD-2154 ?
: .
: : bests regards
: .
------------ End Original Message ------------




 
 Reply 
 
peter
peter
04:39 Dec-13-2006
Re: standard AMS-STD-2154
Can you please send me the AMS-STD-2154 ?
I am very thank you if you do that

sorry I made a mistake of my email

it is xuliang_dy@163.com





 
 Reply 
 
Alfred
Alfred
12:23 Jul-01-2009
Re: standard AMS-STD-2154
In Reply to juan carlos pinzon at 01:17 Jan-29-2003 .

I'd be grateful to receive your pdf file on MIL-STD: 2154 CLASS A

 
 Reply 
 
Dent
Consultant, NDE Manager NDELevel III/3
NDT Consultant, Canada, Joined Nov 1998, 250

Dent

Consultant, NDE Manager NDELevel III/3
NDT Consultant,
Canada,
Joined Nov 1998
250
16:14 Jul-02-2009
Re: standard AMS-STD-2154
In Reply to Russell Austin at 00:08 Jan-24-2003 .

ASTM E2375-08 was developed and adopted to replace MIL STD 2154.

Maybe this will help.

 
 Reply 
 
VICINAY CADENAS, S.A.
VICINAY CADENAS, S.A.
09:17 Oct-23-2009
Re: standard AMS-STD-2154
In Reply to Russell Austin at 00:08 Jan-24-2003 .

Dear Sir,

We have bought the AMS STD 2154 by internet to Techstreet, but they are sending by UPS. Could you send a copy in pdf versión? For us it is very urgent.

Thanks a lot

 
 Reply 
 
Techstreet Customer Service
Techstreet Customer Service
18:12 Oct-23-2009
Re: standard AMS-STD-2154
In Reply to VICINAY CADENAS, S.A. at 09:17 Oct-23-2009 .

"We appreciate your inquiry. We would like to be able to sell ASNT standards in electronic format, but we do not yet have a license agreement from ASNT. We are pursuing an agreement with them, but customers' voices are strong influences. Please feel free to contact Tim Jones or Betsy Blazar at ASNT and tell them you'd like to have their standards distributed through Techstreet. http://www.asnt.org/contact/contact.ihtml

"Of course, there are other NDT standards from ASTM, ISO, and other publishers that we DO sell in print and electronic format."

Visit us anytime at www.techstreet.com

 
 Reply 
 
Rolf
Director,
NDT.net, Germany, Joined Nov 1998, 609

Rolf

Director,
NDT.net,
Germany,
Joined Nov 1998
609
18:58 Oct-23-2009
Re: standard AMS-STD-2154
In Reply to Techstreet Customer Service at 18:12 Oct-23-2009 .

I am wondering why this standard is available for download at SAE.

Download $61.00
Mail $61.00
Fax $61.00

http://www.sae.org/technical/standards/AMSSTD2154

 
 Reply 
 
Megh Pd. Upadhaya
Megh Pd. Upadhaya
12:42 Apr-15-2016
Re: standard AMS-STD-2154
In Reply to juan carlos pinzon at 01:17 Jan-29-2003 .

I will be very much thankful if you could send me a copy of AMS-STD-2154 standard
and i would like to get a Standard practice for Aerospace Ultrasonic standard

 
 Reply 
 

Product Spotlight

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

SONOAIR - air-coupled Phased Array Ultrasonic Inspection System

For highly attenuating materials, the performance of the system is critical. The ultrasonic sensors,
...
the scanning area and the system settings should be flexibly adapted to the test task and the material. These high expectations are met with the new and modular testing system SONOAIR. With the world’s first air-coupled phased-array UT inspection system SONOAIR we developed a technology that works with up to 4 transmitter and receiver channels with freely configurable square wave burst transmitters as wells as low noise receiving amplifiers.
>

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window