Technical Discussions
N. Azarov
Engineering
GosNIIGA, Russia, Joined Jan 2000, 12

N. Azarov

Engineering
GosNIIGA,
Russia,
Joined Jan 2000
12
09:49 Mar-01-2003
about fiberglass construction

Hi, everyone.
Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
N. Azarov


 
 Reply 
 
ISOTEST Engineering S.r.l.
Director
ISOTEST ENGINEERING SRL, Italy, Joined May 2002, 2

ISOTEST Engineering S.r.l.

Director
ISOTEST ENGINEERING SRL,
Italy,
Joined May 2002
2
09:10 Mar-04-2003
re: About fiberglass construction
: Hi, everyone.
: Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
: N. Azarov
.
We have obtained very good results in the control of this materials with air coupled Ultrasounds.
If you want to know more about this "new" methods, please ask.

Bye


 
 Reply 
 
Richard Kazares
Richard Kazares
03:46 Mar-04-2003
Re: re: About fiberglass construction
You might also look at squirter/bubbler (mechanical contour following) techniques using relatively low-cost water-based (recirculation - low volume of water) conventional UT. The advantagesl are that much higher frequencies can be used - resulting in higher resolution images - that are both easier to interpret - as well as providing more detailed information.

Contact me directly - and I'll be happy to e-mail you some honeycomb images taken using this technology and system configuration.

: : Hi, everyone.
: : Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
: : N. Azarov
: .


 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window