00:01 Sep-01-2004
UT standard ETTC 7

Hi,

I am looking for information about the ultrasonic inspection standard ETTC 7. Can anybody tell me what this standard demands or in which book I can find it?

Thanks a lot.

Tamara


 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 183

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
183
06:17 Sep-01-2004
Re: UT standard ETTC 7
reply and question,
Hello,
Are you shure, ETTC7 is a standard on ultrasonic testing (who is the editor)?
ETTC7 looks like Electromagnetic Testing Technical Committee 7;
e.g. the ASTM Committee for Electromagnetic Testing
is numbered ASTM E07.07.

Kind regards
Udo Schlengermann

Applications Laboratory
GE Inspection Technologies Systems GmbH
Tel. +49-2233-601-550
Fax +49-2233-601-402
e-mail udo.schlengermann@ae.ge.com

----------- Start Original Message -----------
: Hi,
: I am looking for information about the ultrasonic inspection standard ETTC 7. Can anybody tell me what this standard demands or in which book I can find it?
: Thanks a lot.
: Tamara
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

On Demand Webinar: Using Eddy Current Array for Large Areas in Place of Magnetic Particle and Liquid Penetrant Testing

New on-demand webinar on the use of eddy current array (ECA) technology in lieu of liquid penetrant
...
testing (PT) and magnetic particle testing (MT) for large area screenings. The webinar includes an introduction to the technologies with advantages and disadvantages of each. Side by side examples are discussed including aircraft stringers, engine blades, forgings, weld plates & more. View it today.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window