High Temp Liq. Pen (Nuclear)

Does anyone know of any high temperature liquid penetrant chemicals that are certified for use on nuclear components?

Basically if they meet ASME section V for sulfer and halogen content then they are ok for nuclear.

Anyone know????


 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
03:34 Feb-26-2006
Re: High Temp Liq. Pen (Nuclear)
Dear Scott,

How high do you want to go?

Swamy

----------- Start Original Message -----------
: Does anyone know of any high temperature liquid penetrant chemicals that are certified for use on nuclear components?
: Basically if they meet ASME section V for sulfer and halogen content then they are ok for nuclear.
: Anyone know????
------------ End Original Message ------------




 
 Reply 
 
Scott
Scott
09:31 Mar-02-2006
Re: High Temp Liq. Pen (Nuclear)
I see flash point of most high temp penetrants is 200 deg C, that would be fine.

Do you know of any accepted for nuclear use?


----------- Start Original Message -----------
: Dear Scott,
: How high do you want to go?
: Swamy
: : Does anyone know of any high temperature liquid penetrant chemicals that are certified for use on nuclear components?
: : Basically if they meet ASME section V for sulfer and halogen content then they are ok for nuclear.
: : Anyone know????
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window