pscan

Could somebody enlighten me about pscan. Is it the same as tofd?


 
 Reply 
 
S. Gripp
S. Gripp
02:20 Jul-07-1999
Re: pscan
pscan is a mechanised UT system from FORCE-Denmark (trade name for 'projection scan')
tofd is 'time of flight diffraction' technique, a method to detect flaws by their diffraction
signal rather than by reflection.

So, one is a system, the other is a method.
pscan can "tofd", so can many others.



 
 Reply 
 
pramod myakal
Consultant
AGM Techno consultants, India, Joined Jan 2003, 22

pramod myakal

Consultant
AGM Techno consultants,
India,
Joined Jan 2003
22
08:13 Sep-05-1999
Re: pscan
: pscan is a mechanised UT system from FORCE-Denmark (trade name for 'projection scan')
: tofd is 'time of flight diffraction' technique, a method to detect flaws by their diffraction
: signal rather than by reflection.

: So, one is a system, the other is a method.
: pscan can "tofd", so can many others.




 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window