where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

ULTRASOUND INSTITUTE
The Ultrasound Institute can develop new advanced ultrasonic measurement, imaging and NDT techniques for non-conventional applications.
3228 views
Technical Discussions
Sunny
Sunny
05:02 Jun-21-2006
UT Immersion system

Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide

Thanks


 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:25 Jun-21-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

We, Mahindra Intertrade Ltd has built many Immersion Tank systems for various Customers in India. We can supply Manipulators, Electronics, Software etc., depends on application and Customer reqts.

For further details, contact us.

Regards.

D.Simon Amallraja


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
05:19 Jun-22-2006
Re: UT Immersion system
This is the link for Midas (ex-Meccasonics people) who manufacture immersion systems in the UK:

www.midas-ndt.co.uk

----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------




 
 Reply 
 
Athanasios Anastasopoulos
Director,
Mistras Group, Greece, Joined Jan 2000, 14

Athanasios Anastasopoulos

Director,
Mistras Group,
Greece,
Joined Jan 2000
14
03:44 Jun-22-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

Have a look at the following manufacturers:

http://www.ndtautomation.com

http://www.olympusndt.com

We develope and supply analysis and evaluation s/w, UTIA, specially designed for immersion systems. For additional info please visit www.envirocoustics.gr or specifically for UTIA
http://www.envirocoustics.gr/software/utia/utia_eng.htm



 
 Reply 
 
Phil Thayer
Phil Thayer
04:44 Jun-22-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

We, NDT Automation manufacture a full range of immersion systems from small lab systemss to large industrial scanners. NDTA manufactures our own UT system cards (including GE approval for disc inspection). Please visit our web site at www.ndtautomation.com


 
 Reply 
 
Shmuel Saitowitz
Shmuel Saitowitz
05:46 Jun-22-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

ScanMaster Systems is the world's leader in the supply of ultrasonic inspection systems with over 300 installations world wide. ScanMaster has approvals from the large aerospace manufactures such as GEAE, Rolls Royce, MTU, Snecma and Pratt & Whitney. Systems are installed at customers like GE, Pratt & Whitney, Aubert Duvall/Fortech, MTU, TEI, Denel Aerospace, Boeing, Wyman Gordon, Boeing, amongst many others.

ScanMaster has local representation all over the world and service and support in all countries where installations have taken place.





 
 Reply 
 
Patrick Louviot
Patrick Louviot
08:38 Jun-23-2006
Re: UT Immersion system
----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------

You can try www.metalscan.fr
Metalscan is a UT specialist since 1985.



 
 Reply 
 
James Dolfi
Director
ford, USA, Joined Oct 1999, 8

James Dolfi

Director
ford,
USA,
Joined Oct 1999
8
05:51 Jun-23-2006
Re: UT Immersion system
----------- Start Original Message -----------
: : Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: : Thanks
: You can try www.metalscan.fr
: Metalscan is a UT specialist since 1985.
------------ End Original Message ------------


You can get more information at applied metrics.
They have made systems to check spot welds and material properties etc. Marv Fleming is the President of this company mail mmf@applied-metrics.com.

Hope this helps.



 
 Reply 
 
K S Lakshmanan
K S Lakshmanan
07:25 Jun-24-2006
Re: UT Immersion system
Dear Sir,

We would like to inform that we are the authorized / exclusive Representative of Olympus NDT for their complete range of Products in India (Panametrics NDT (U.S.A.), R/D Tech (Canada), Staveley NDT (U.S.A.) are the business units of Olympus NDT).

We had supplied many ultrasonic immersion systems in INDIA.

We request you to please let us know your requirement in detail, full address, contact phone numbers to enable us to submit our Offer.

Best Regards

K.S.Lakshmanan,

General Manager

Testing Machines Department

Blue Star Limited

No. 46, Cathedral Road

Chennai - 600 086

Direct No. 0091 44 4244 4250

Mobile No. 99400 36849

Board No. 0091 44 4244 4000

Fax No. 0091 44 4244 4190 / 0091 44 28116736

----------- Start Original Message -----------
: Could anyone give me suggestion on which company has reliable ut immersion systems?anyone having experience with GE, Matech or other systems? Please guide
: Thanks
------------ End Original Message ------------




 
 Reply 
 
David LAVASTRE
David LAVASTRE
05:47 Jun-24-2006
Re: UT Immersion system
Hi Sunny,
Many manufacturers can provide UT systems qualified following GEAE specs.
With GEAE specifications, the UT systems (instrument+transducers) must be registered in a "Data For Ordering" file and you can use only transducers and instrument that are in DFOs.
Also, The "tank" must met with GEAE specs geometric requirements.
The manufacturers that are already qualified that I know are ;
Matec (USA)> http://www.matec.com/
IRT Scanmaster (Israel)> http://www.scanmaster-irt.com/
BIA (France > http://www.bia.fr/
GE Inspection Technologies (USA)>http://www.geinspectiontechnologies.com/index.html

For the instruments and transducers, and for conventional immersion UT, GEAE suppliers use ;
Harisonic transducers (now Olympus NDT) > http://www.olympusndt.com/
Megasonic IHM and TLC transducers.

I think that you can ask for DFOs to Mr Thadd Patton at thadd.patton@ae.ge.com

David



 
 Reply 
 
Tristian
Tristian
07:36 Nov-27-2006
Addison
Hello%2C+nice+site+look+


 
 Reply 
 

Product Spotlight

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window