where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
EWGAE 2012 |Website| by NDT.net

30th European Conference on Acoustic Emission Testing & 7th International Conference on Acoustic Emission at University of Granada, 12-15 September 2012

Share ...     

Keywords Authors & Institutions
Search Results: 2 in Date '2012-11-01'      Search  
Title / Author(s) / Keywords Session
AE in Wood and Biological Applications
Correlation of Sap Flow Changes in Trees with Signal of Acoustic Emission during Field Measurements
P. Mazal155, M. Cerny26, F. Vlašic126, L. Nohál111
1aFaculty of Mechanical Engineering(FME) bFaculty of Mechanical Engineering; Brno University of Technology (BUT)224, Brno, Czech Republic
2Agronomická fakulta; Mendel University in Brno (MZLU Brno)7, Brno, Czech Republic
Acoustic Emission (AE), Acoustic Emission (AE), AE Sensors, trees, SAP flow

AE in Wood and Biological Applications
Poster Presentations
Monitoring and Evaluation of Cyclic Damage in Preinitiation Stages of Fatigue Process Using Nondestructive Testing Methods
F. Vlašic126, V. Koula28, P. Mazal155, P. Gejdoš13
1aFaculty of Mechanical Engineering bFaculty of Mechanical Engineering(FME); Brno University of Technology (BUT)224, Brno, Czech Republic
2Center Dakel; ZD Rpety-Dakel10, Prague, Czech Republic
fatigue damage, crack, Acoustic Emission (AE), microstructural changes