Applications of Continuous Sampling of AE Signal for Detection of Fatigue Damage
P. Mazal155, V. Koula28, F. Hort114, F. Vlašic126
1Faculty of Mechanical Engineering; Brno University of Technology (BUT)227, Brno, Czech Republic
2ZD Rpety-Dakel10, Prague, Czech Republic
Acoustic Emission (AE), early damage detection, bearing, Fatigue, contact fatigue

   