1999-02
Mechanized Ultrasonic Inspection of Large Diameter Gas Pipeline Girth Welds
N. Dube13, E. Ginzel299, M. Moles †2014147
1Olympus Scientific Solutions Americas (OSSA)232, Waltham, MA, USA
2Materials Research Institute102, Waterloo, Canada
Ultrasonic Testing (UT), chemical & petrochemical, weld