Phased Arrays for Small Diameter, Thin-Walled Piping Inspections
M. Moles †2014147, E. Ginzel299
1Olympus Scientific Solutions Americas (OSSA)232, Waltham, MA, USA
2Materials Research Institute102, Waterloo, Canada
Ultrasonic Testing (UT), phased array, automated ultrasonic testing (AUT), tubes and pipes, weld
   