2017-10 Journal-AE, Volume 34, 2016
Influence of pre-compression on tensile behavior in wrought AZ31 studied by the acoustic emission technique
D. Drozdenko1, P. Dobron1, J. Bohlen2, S. Yi2, F. Chmelík12
1Department of Metal Physics; Charles University8, Prague, Czech Republic
2Helmholtz-Zentrum Geesthacht6, Geesthacht, Germany

 
Journal-AE
Session: Volume 34, 2016
2017-10
2012-11 Journal-AE, Volume 20, 2003
Acoustic Emission from Magnesium-Based Alloys and Metal Matrix Composites
F. Chmelík12, F. Moll2, J. Kiehn2, K. Mathis32, P. Lukác1, K. Kainer4, T. Langdon5
1Department of Metal Physics; Charles University8, Prague, Czech Republic
2Clausthal University of Technology 5, Clausthal-Zellerfeld, Germany
3Department of General Physics; Eötvös Loránd University, Budapest, Hungary
4Institute for Materials Research; GKSS-Forschungszentrum Geesthacht GmbH2, Geesthacht, Germany
5University of Southern California4, Los Angeles, CA, USA
Acoustic Emission (AE)
 
Journal-AE
Session: Volume 20, 2003
2012-11
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window