Aerospace
Ultrasonic Non-Destructive Inspection of Localized Porosity in Composite Materials
N. Dominguez28, B. Mascaro
AIRBUS OPERATIONS SAS22, Toulouse, France
Ultrasonic Testing (UT), Aerospace, composite, carbon fiber reinforced plastic (CFRP), porosity, structural noise analysis