Report on thickness measurement of basis metal through paint and compound coatings using Ultrasonic Thickness Gauge А1210

Acoustic Control Systems Ltd.20, Moscow, Russia

Our engineers checked and proved the possibility of measuring basis metal thickness through paint and compound coatings processing good adhesion to metal using ultrasonic thickness gauge A1210.

Goal of research: Assessment of capability for thickness measurements of metals through coatings possessing good adhesion to metal.

Object of research: A segment of the steel plate with a paint coating on one side and a compound coating on the other side.

Instrument used for research: Ultrasonic Thickness Gauge А1210 with A-SCAN operating mode and double crystal transducer D1771 with 4 MHz operating frequency.

Accessories: A special-purpose gel for ultrasonic thickness measurements of different structural material.

The report is available by following the Link

 
Visit: Acoustic Control Systems Ltd.

Feedback: ()

Share:
More from "Acoustic Control Systems Ltd." (5 of 20)
2017-02Acoustic Control Systems - ACS Group has founded a new company in Germany – ACS-Solutions GmbH
2017-01Acoustic Control Systems Ltd. celebrated 25 year anniversary
2016-10Special purpose holder for low frequency DPC transducers S18 series
2016-08Acoustic Control Systems Ltd. has expanded types of low frequency dry point contact transducers
2016-06Acoustic Control Systems Ltd. continue developing the area of equipment for automated inspection of the pipelines
... All 20 Details >
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window